在常温常压下,以硝酸钙(Ca(NO3)2·4H2O)和磷酸氢二铵((NH4)2HPO4)为原料,运用超声喷雾法技术制备了羟基磷灰石(HAP)纳米粉体,获得了颗粒度为30~40nm的均匀HAP粉体.研究了化学反应时间与烧结温度对HAP的结晶度和颗粒均匀性的影响规律.在相同的制备工艺条件下,与传统的超声化学法和化学沉淀法制得的HAP粉体样品进行比较,发现超声喷雾法可以在较短的反应时间内制备出纳米HAP,显著提高HAP的合成效率、结晶度,且获得的颗粒度相对均匀.

参考文献

[1] 刘光华.现代材料化学[M].上海:上海科学技术出版社,2000:512-517.
[2] Webster TJ;Ergun C;Doremus RH;Siegel RW;Bizios R .Enhanced osteoclast-like cell functions on nanophase ceramics.[J].Biomaterials,2001(11):1327-1333.
[3] Deng X;Hao J;Wang C .Preparation and mechanical properties of nanocomposites of poly(D,L-lactide) with Ca-deficient hydroxyapatite nanocrystals.[J].Biomaterials,2001(21):2867-2873.
[4] Kikuchi M;Itoh S;Ichinose S;Shinomiya K;Tanaka J .Self-organization mechanism in a bone-like hydroxyapatite/collagen nanocomposite synthesized in vitro and its biological reaction in vivo.[J].Biomaterials,2001(13):1705-1711.
[5] 郑昌琼;冉均国.新型无机材料[M].北京:科学出版社,2003
[6] LIU H S;CHlN T S;LAI L S et al.Hydroxyapatite synthesized by a simplified hydrothermal method[J].Ceramics International,1997,23:19-25.
[7] Bezzi G.;Celotti G.;Landi E.;La Torretta TMG.;Sopyan I.;Tampieri A. .A novel sol-gel technique for hydroxyapatite preparation[J].Materials Chemistry and Physics,2003(3):816-824.
[8] CHAI C S;BEN-NISSAN B .Bioactive nanocrystalline sol-gel hydroxyapatite coatings[J].Journal of Materials Science:Materials in Medicine,1999,10(08):465-469.
[9] FURUZONO T;WALSH D;SATO K .Effect of reaction temperature on the morphology and size of hydroxyapatite nanoparticle in an emulsion system[J].Journal of Materials Science Letters,2001,20(01):111-114.
[10] LIN G K;WANG J .Formation of nanohydroxyapatite in nonionic emulsion[J].Langmuir,1995,15:7472-7477.
[11] LIMIN Q;JIMING M.Microemulsion-mediated synthesis of calcium hydroxyapatite fine poweder[J].Journal of Materials Science Letters,1997(16):1779-1781.
[12] MURRAY M G S;PONTON C B;MARQUIS P M .Processing of uhrafine grained hydroxyapatite bioceramics britain ceramic processings[J].Nanoceramics,1993,51:25-30.
[13] 王志强,马铁成,蔡英骥,韩趁涛,吕秉玲.湿法合成纳米羟基磷灰石粉末的研究[J].无机盐工业,2001(01):3-5.
[14] Tas AC .Synthesis of biomimetic Ca-hydroxyapatite powders at 37 degrees C in synthetic body fluids.[J].Biomaterials,2000(14):1429-1438.
[15] YAMAGUCHI I;TOKUCHI K;PUKUZAKI H .Preparation and microstructure analysis of chitosan/hydroxyapatite nanocomposites[J].Journal of Biomedical Materials Research,2000,55(01):20-27.
[16] 黄立业,徐可为.纳米针状羟基磷灰石涂层的制备及其性能的研究[J].硅酸盐学报,1999(03):351-356.
[17] Shirkhanzadeh M. .Direct formation of nanophase hydroxyapatite on cathodically polarized electrodes[J].Journal of Materials Science. Materials in Medicine,1998(2):67-72.
[18] 陈际达,王远亮,蔡绍皙,曹颖.纳米羟基磷灰石/胶原复合材料制备方法研究[J].生物物理学报,2001(04):778-784.
[19] 林开利,成荣明,常江.超声化学法合成纳米羟基磷灰石粉体的研究[J].材料导报,2006(z2):182-184.
[20] SUSLIC K S .Sonochemistry[J].Science,1990,247:1439.
[21] 华缜,靳正国,程志捷.超声条件下羟基磷灰石纳米针状晶体的制备[J].材料导报,2003(z1):75-77.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%