高级检索

采用激光立体成形技术制备GH4169高温合金块体,对其在720~780℃温度区间进行不同保温时间的双级时效处理,采用微观测试分析方法对高温短时时效处理后γ"相的形态、尺寸变化及粗化动力学行为进行研究.结果表明:激光立体成形GH4169合金在不同保温时间双级时效条件下,γ"相形态基本为圆盘形;和保温时间相比,时效温度对γ"相的影响更为显著;γ"相的粗化规律符合Lifshitz Slyozov Wagner(LSW)理论,计算获得γ"的粗化激活能Q=281.85kJ/mol,较锻造GH4169合金的γ"粗化激活能略高,表明激光立体成形GH4169合金的组织稳定性优于锻态.

参考文献

[1] LI M Q,JU W B,LIN Y Y,et al .Deformation behavior of GH4169 nickel based superalloy in isothermal compression[J].Material Science andTechnology,2008,24(10):1195-1198.,2008.
[2] RAO G A,KYMAR M,SRINIVAS M,et al .Effect of standard heat treatment on the microstructure and mechanical properties of hot isostatically pressed superalloy Inconel 718[J].Materials Sci ence and Engineering:A,2003,355:114-125.,2003.
[3] 白秉哲,杨鲁义,赵耀峰.GH4169 合金"等温锻造+直接时效"工艺探讨[J].稀有金属,2002(01):7-11.
[4] OBLAK J M,PAULONIS K F,DUVALL D S .Coherency strengthening in Ni base alloys hardened by DO22 γ" precipitates[J].Metallurgical Transactions A,1974,5(1):143-153.,1974.
[5] MAHONEY M W.Superplastic properties of alloy 718[A].Su peralloy 718 Metallurgy and Applications[C].USA:The Miner als,Metals & Materials,1989.391-405.,1989.
[6] 呼和.镍基铸造高温合金的热等静压处理[J].金属学报,2002(11):1199-1202.
[7] 王淑云,李惠曲,李辉忠,计晟,崔健.FGH95合金等温锻造工艺研究[J].稀有金属,2003(04):452-454.
[8] 黄卫东,林鑫.激光立体成形高性能金属零件研究进展[J].中国材料进展,2010(06):12-27.
[9] 黄卫东,林鑫,陈静,等.激光立体成形[M].西安:西北工业大学出版社,2007.HUANG Wei-dong,LIN Xin,CHEN Jing,et al.Laser Solid Forming[M].Xi'an:Northwestern Polytechnical University Press,2007.,2007.
[10] KNOROVSKY G A,CIESLAK M J,HEADLEY T J,et al .Inconel 718:a solidification diagram[J].Metallurgical and Ma terials Transactions A,1989,20(10):2149-2158.,1989.
[11] SUNDARARAMAN M,MUKHOPADHYAY P,BANERJEE S .Some aspects of the precipitation of metastable intermetallic phases in Inconel 718[J].Metallurgical and Materials Transac tions A,1992,23(7):2015-2028.,1992.
[12] 朱景川,来忠红.固态相变原理[M].北京:科学出版社,2010.ZHU Jing-chuan,LAI Zhong-hong.Solid Phase Transformation Principle[M].Beijing:Science Press,2010.,2010.
[13] J.H. Du,X.D. Lü,J.L. Qu,Q. Deng,J.Y. Zhuang,Z.Y. Zhong.MICROSTRUCTURE AND MECHANICAL PROPERTIES OF NOVEL 718 SUPERALLOY[J].金属学报(英文版),2006(06):418-424.
[14] DONG Jian xin,XIE Xi-shan,ZHANG Shou hua .Coarsening behavior of γ" precipitates in modified inconel718 superalloy[J].Scripta Metallurgica et Materialia,1995,33(12):1933-1940.,1995.
[15] DEVAUXSA,NAZE L,MOLINS R,et al .Gamma double prime precipitation kinetic in alloy 718[J].Materials Science and Engineering:A,2008,486:117-122.,2008.
[16] HE J H,TANG X Y,FUKUYAMA S .Boundary in γ" precipi tates in Inconel 718 nickel-base superalloy[J].Acta Metall Ma ter,1995,43(12):4403-4409.,1995.
[17] LIFSHITZ I M,SLYOZOV V V .The kinetics of precipitation from supersaturated solid solutions[J].Journal of Physics and Chemistry of Solids,1961,19:35-50.,1961.
[18] CALDERON H A,FINE M E .Coarsening kinetics of coherent NiAl type precipitates in Fe-Ni-Al and Fe-Ni-Al-Mo alloys[J].Materials Science and Engineering,1984,63(2):197-208.,1984.
[19] LI X,SAUNDERS N,MIODOWNIK A P .The coarsening ki netics of γ' particles in nickel based alloys[J].Metallurgical and Materials Transactions A,2002,33(11):3367-3373.,2002.
[20] CALDERON H A,KOSTORZ G,QU Y Y,et al .Coarsening kinetics of coherent precipitates in Ni-Al-Mo and Fe-Ni-Al alloys[J].Materials Science and Engineering:A,1997,238(1):13-22.,1997.
[21] MAO J.Gamma prime precipitation modeling and strength re sponses in powder metallurgy superalloys[D].West Virginia:West Virginia University,2002.,2002.
[22] DEVAUX A,NAZE L,MOLINS R,et al .Gamma double prime precipitation kinetic in alloy 718[J].Materials Science and Engineering:A,2008,486:117-122.,2008.
[23] KARUNARATNE M S A,REED R C .Interdiffusion of niobi um and molybdenum in nickel between 900 1300℃[J].Defect and DiffusionForum,2005,237