以 SR、纳米 Fe3 O4和纳米 MH 为主要原料制备 MH/Fe3 O4/SR 磁性橡胶复合材料。研究纳米 Fe3 O4和纳米 MH不同配比时,复合材料的物理力学性能变化、耐热以及摩擦性能变化。结果表明:纳米粒子在 SR 基体中分布较为均匀,不同配比的 Fe3 O4/MH 能够有效改善硅橡胶的物理力学性能。当配比20phrMH/10phrFe3 O4时,复合材料的拉伸强度、伸长率有所改善,性能较普通硅橡胶提高了5%左右。随着纳米 MH 与 Fe3 O4填料填充量不断加大,复合材料耐热性能不断提高,摩擦因数有效降低。当纳米添加量为30phrMH/10phrFe3 O4时,复合材料的分解温度提高为450℃,当纳米添加量为20phrMH/20phrFe3 O4时,复合材料的摩擦因数降为0.52。

The MH/Fe3 O4/SR magnetic rubber composites were prepared with SR,nano-Fe3 O4 and nano-MH as raw materials.The friction,heat-resistant,physical and mechanical properties of the MH/Fe3 O4/SR composites were studied using different proportions of nano-Fe3 O4 and nano-MH.The results show that nano particles are well distributed in the silicone rubber matrix.The physical and mechanical properties of silicone rubber are effectively improved by different ratios of Fe3 O4/MH. When the ratio is 20phrMH/10phrFe3 O4 ,the tensile strength and elongation of the composites are somewhat improved,increase by 5%,compared with common silicone rubber.With the increase of the addition of nano MH and Fe3 O4 ,the heat-resistant and friction properties of composites are continu-ously improved, the friction coefficient is effectively demoted. When the ratio is 30phrMH/10phrFe3 O4 ,the decomposition temperature of the composites increases to 450℃.When the ratio is 20phrMH/20phrFe3 O4 ,the friction coefficient of the composites is demoted to 0.52.

参考文献

[1] 傅政.橡胶材料性能与设计应用[M].北京:化学工业出版社,2003
[2] K. H. Prema;Philip Kurian;P. A. Joy .Physicomechanical and Magnetic Properties of Neoprene Based Rubber Ferrite Composites[J].Polymer-Plastics Technology and Engineering,2008(1/3):137-146.
[3] 刘继纯,常海波,李晴媛,陆昶,潘炳力,杜西刚.Mg(OH)2/聚苯乙烯复合材料的阻燃机制[J].复合材料学报,2012(05):32-40.
[4] TAGUETA A;CASSAGNAUB P;LOPEZ J M et al.Structur-ation,selective dispersion and compatibilizing effect of nano-fillers in polymer blends[J].Progress in Polymer Science,2014,39(08):1526-1563.
[5] LAETITIA M;OLIVER C;MICHAL K et al.Implementation of metal-free ring-opening polymerization in the preparation of ali-phatic polycarbonate materials[J].Progress in Polymer Science,2014,39(06):1144-1164.
[6] 张春梅,杜华太,庞明磊,张志刚,崔俞,杜明欣,张洪民,陈斌.有机蒙脱土/氢化丁腈橡胶纳米复合材料的结构和性能[J].航空材料学报,2013(05):66-71.
[7] PATTANA K;PONGDHOM S;NiITTAYA R .Mechanical and electrical properties of natural rubber and nitrile rubber blends filled with multi-wall carbon nanotube:Effect of preparation methods[J].Polymer Testing,2013,32(04):731-738.
[8] 胡晓.Fe3O4/聚乙烯磁性复合材料的阻燃性能研究[J].消防科学与技术,2012(02):171-173.
[9] HE S J;WANG Y Q;XI M M et al.Prevention of oxide aging acceleration by nano-dispersed clay in styrene-butadiene rubber matrix[J].Polymer Degradation and Stability,2013,98(09):1773-1779.
[10] RAJASEKAR R;KAUSHIK P;GERT H et al.Development of nitrile butadiene rubber-nanoclay composites with epoxidized natural rubber as compatibilizer[J].Materials and Design,2009,30(09):3839-3845.
[11] YU H Y;ZHANG Y;CHEN S G et al.Study on the proper-ties of ethylene-vinyl acetate rubber vulcanizate filled with super-fluous magnesium hydroxide/methacrylic acid[J].Journal of Applied Polymer Science,2011,119(03):1813-1819.
[12] 庞佑霞,许焰,张昊,唐勇,刘厚才.微/纳米复合涂层的抗冲蚀磨损性能[J].材料工程,2013(09):60-63.
[13] 沈尔明,李晓欣,王志宏,滕佰秋,刘嘉.长期储存后橡胶材料湿热老化分析[J].材料工程,2013(07):87-91.
[14] WANG X J;CHI Y L;LIU H B et al.Research on the impact and friction and wear properties of acrylonitrile-butadiene-rubber composites filled with SiC and graphite[J].Journal of Thermo-plastic Composite Materials,2014,27(08):1013-1021.