饱水木质文物在世界各地均有发现,其保护引起了广泛重视。从出土饱水木质文物存在的腐蚀病害类型及保护研究方面综述了目前国内外这一领域的研究进展。对现有保护方法存在的问题进行了详细分析,并展望了未来的研究重点和发展方向。

The archaeological waterlogged wooden artifacts have been found around the world,and their con-servation attracted wide attention.The progress of conservation on waterlogged wooden artifacts at home and abroad are reviewed mainly from the corrosion types and conservation methods.The problems of existing conservation me-thods for waterlogged wooden artifacts are analyzed in detail,and the prospect of conservation methods is presented.

参考文献

[1] Rowell.Structure and degradation process for waterlogged archaeological wood[M].Washington:American Chemical Society,1990:35.
[2] Guichen G D.Conservation on archaeological excavations[M].Rome:ICCROM,1995:23.
[3] Bj?rdal C G;Nilsson T .Waterlogged archaeological wood-A substrate for white rot fungi during drainage of wetlands[J].Intl Biodeterior Biodegrad,2002,50:123.
[4] 陈家昌,郑元锁.水溶性丙烯酸树脂在出土饱水漆木器脱水定型中的应用研究[J].文物保护与考古科学,2005(03):28-34.
[5] Gianna Giachi;Chiara Capretti;Nicola Macchioni .A me-thodological approach in the evaluation of the efficacy of treatments for the dimensional stabilization of waterlogged archaeological wood[J].J Cultural Heritage,2010,11:91.
[6] 李国清.出土饱水古木件干缩性探讨[A].北京,1987:70.
[7] Leszek Babiński;Dorota Izdebska-Mucha;Bogus?awa Waliszewska.Evaluation of the state of preservation of waterlogged archaeological wood based on its physical properties: basic density vs. wood substance density[J].Journal of Archaeological Science,2014:372-383.
[8] David Hunt .Properties of wood in the conservation of his-torical wooden artifacts[J].J Cultural Heritage,2012,13S:10.
[9] 胡继高;马箐毓.考古出土饱水竹、木、漆器脱水保护[J].中国文化遗产,2003(3):59.
[10] 邬义明.植物纤维化学[M].北京:中国轻工业出版社,1991
[11] Chen Jiachang et al.Shape recovering from collapsed ar-chaeological waterlogged wood by active alkali-urea treat-ment[J].JOURNAL OF ARCHAEOLOGICAL SCIENCE,2009,36:434.
[12] Oddy W A .Chemistry in the conservation of archaeological materials[J].Science of the Total Environment,1994,121:143.
[13] 陈中行.饱水竹器的保护和脱水动力学[A].北京,1987
[14] 成俊卿;蔡少松.木材识别与利用[M].北京:中国林业出版社,1982:56.
[15] 胡东波,胡一红.考古出土饱水木器的腐朽、收缩变形原理[J].文物,2001(12):80-85.
[16] 陈庚龄,卢燕玲.甘肃出土糟朽木器环境腐蚀作用与机理研究[J].文物保护与考古科学,2009(04):67-73.
[17] 马菁毓.饱水古木材的结构和降解过程[J].东南文化,2004(01):91-96.
[18] 罗曦芸 .饱水文物传统脱水方法与超临界流体干燥技术的应用[J].文物保护与考古科学,2002,14(S1):101.
[19] Magnus S;Farideh J;Ingmar P et al.Deterioration of the seventeenth century warship Vasa by internal formation of sulphuric acid[J].NATURE,2002,415:893.
[20] Magnus S;Farideh J;Emiliana D et al.Sulfur accumula-tion in the timbers of King Henry VIII′s warship Mary Rose:A pathway in the cycle of conservation concern[J].Proceedings of the National Academy of Sciences(USA),2005,102(40):14165.
[21] Yvonne Fors;Magnus Sandstr?m .Sulfur and iron in shipw-recks cause conservation concerns[J].CHEMICAL SOCIETY REVIEWS,2006,35:399.
[22] 马丹,郑幼明.“华光礁一号”南宋沉船船板中硫铁化合物分析[J].文物保护与考古科学,2012(03):84-89.
[23] Wetherall K M;Moss R M;Jones A M et al.Sulfur and iron speciation in recently recovered timbers of the Mary Rose revealed via X-ray absorption spectroscopy[J].J Ar-chaeol Sci,2008,35:1317.
[24] Robert B .A review of microbial deterioration found in ar-chaeological wood from different environments[J].Int Bio-deter Biodegrad,2000,46:189.
[25] Brian A Jordan .Site characteristics impacting the survival of historic waterlogged wood:A review[J].Int Biodeter Bio-degrad,2001,47:321.
[26] Ferrari B;Adams J .Biogenic modification of marine sedi-ments and their influence on archaeological materials[J].Int J Nautical Archaeol,1990,19(3):139.
[27] Nicola Macchioni .Physical characteristics of the wood from the excavations of the ancient port of Pisa[J].J Cultural Heritage,2003,32(4):85.
[28] 赵桂芳;嵇益民;马箐毓.探究用聚乙二醇处理饱水古代湿木色泽变化的原因[J].文物科技研究,2006(2):127.
[29] 张金萍.考古木材的变色与脱色研究[A].北京,2004:39.
[30] Fors Y;Richards V .The effects of the ammonia neutralizing treatment on marine archaeological vasa wood[J].Stud Con-serv,2010,55:41.
[31] Rodorico Giorgi;David Chelazzi;Emiliano Fratini et al.Nanoparticles of calcium hydroxide for wood deacidification:Decreasing the emissions of organic acid vapors in church or-gan environments[J].J Cultural Heritage,2009,10:206.
[32] 田兴玲;李乃胜;张治国 等.文物自动清洗脱盐系统的仿真与优化[J].环境工程,2014,32(S1):1055.
[33] 张治国,李乃胜,田兴玲,刘婕,沈大娲.宁波“小白礁Ⅰ号”清代木质沉船中硫铁化合物脱除技术研究[J].文物保护与考古科学,2014(04):30-38.
[34] Mikkel C;Hartmut K;Finn H .New materials used for the consolidation of archaeological wood-past attempts,present struggles,and future requirements[J].J Cultural Heritage,2012,13S:183.
[35] Charlotte Gjelstrup Bj?rda .Microbial degradation of water-logged archaeological wood[J].J Cultural Heritage,2012,135:S118.
[36] Uppsala S .Microbial decay of waterlogged archaeological wood found in Sweden:Applicable to archaeology and con-servation[J].Int Biodeter Biodeg,1999,43(1-2):63.
[37] 胡东波,宋少华,肖静华.长沙走马楼出土饱水竹简的防腐保存[J].文物保护与考古科学,2003(02):14-19.
[38] 陆衡.绍兴印山大墓木椁毒菌的硫酰氟杀灭实验[A].荆州,2005:375.
[39] 赵桂芳,孙延忠,马箐毓,刘秀英,陈允适.防霉防腐剂的抗流失性及防霉效果的研究[J].文物保护与考古科学,2006(01):1-3.
[40] Hoffmann P E R .On the stabilization of waterlogged wood with PEG Ⅱ.Designing two step treatment for multi-quali-ty timbers[J].Stud Conserv,1986,31:103.
[41] Chaumat Gilles.Trials of shape recovering from collapsed waterlogged wood by treatment with carbon dioxide(CO2)supercritical fluid[A].Bre-merhaven,1999:137.
[42] 陈家昌;周敬恩;柴东朗 等.干缩变形木质文物的润胀复原研究[J].功能材料,2009,41(8):1450.
[43] 方北松,吴顺清.饱水竹木漆器保护修复的历史、现状与展望[J].文物保护与考古科学,2008(z1):122-130.
[44] 刘秀英,陈允适.木质文物的保护和化学加固[J].文物春秋,2000(01):50-59.
[45] 曹盛葆.关于出土漆竹木器的保养保护[A].北京,1987:33.
[46] 李文英.对九件汉代饱水漆木器脱水定形实验报告[A].北京,1987:40.
[47] 刘丽,李文英,杨竹英.硅胶在出土浸饱水漆木器脱水定型中的应用与研究[J].文物保护与考古科学,2005(02):39-41.
[48] 张立明,黄文川,何爱平,金普军.自然干燥法在保护西汉饱水漆耳杯中的应用[J].文物保护与考古科学,2005(04):44-47.
[49] 陈元生;解玉林 .严重朽蚀饱水竹简的真空冷冻干燥研究[J].文物保护与考古科学,1999,11(1):5.
[50] 张绍志;房圆圆;陈光明 等.文物冷冻十燥水蒸气扩散系数的测量[J].化工学报,2012,63(S1):28.
[51] 刘博.漆木耳杯真空速冻干燥及加固处理[J].北方文物,2005(04):104-107.
[52] Jensen J B .Dynamic model for vacuum freeze-drying of wa-terlogged archaeological wooden artefacts[J].J Cultural Heritage,2006,7:156.
[53] Samuel P;Nigel K H Slater;Mark Jones et al.Investiga-ting the processes necessary for satisfactory freeze-drying of waterlogged archaeological wood[J].JOURNAL OF ARCHAEOLOGICAL SCIENCE,2009,36(4):2177.
[54] 张金萍.用甘露醇和 PEG 保护饱水木质文物的冷冻干燥法[J].东南文化,1996(4):127.
[55] Leszek Babinski .Investigations on pre-treatment prior to freeze-drying of archaeological pine wood with abnormal shrinkage anisotropy[J].JOURNAL OF ARCHAEOLOGICAL SCIENCE,2011,38(2):1709.
[56] 胡继高.银雀山和马王堆出土竹简脱水试验报告[J].文物,1979(4):64.
[57] 赵桂芳.醇-醚联浸法的探讨[A].北京,1987:42.
[58] 陈中行,程丽臻,李澜.乙二醛脱水加固定型曾侯乙墓和包山楚墓彩漆主棺[J].文博,2009(06):463-467.
[59] 罗曦芸.乙二醛用于加固饱水漆木器的研究[J].化学世界,2001(03):134-137,164.
[60] Martin N M;Helge E;Soren H et al.Characterisation of the polyethylene glycol impregnation of the Swedish warship Vasa and one of the Danish Skuldelev Viking ships[J].JOURNAL OF ARCHAEOLOGICAL SCIENCE,2007,34:1211.
[61] 韦荃,金普军,岡田文男,吉田秀男.四川省绵阳市永兴双包山西汉墓出土漆、木器文物保护研究[J].文物保护与考古科学,2004(02):39-44.
[62] 陈进良;崔战华 .河南信阳长台关出土的饱水漆木器脱水定研究报告[J].文物保护与考古科学,1994,6(2):1.
[63] 卢衡,刘莺,靳海斌,刘东坡.置换填充法稳定浙江安吉出土饱水木俑的研究[C].中国文物保护技术协会第六次学术年会论文集,2009:94-101.
[64] Barry Kaye;David J. Cole-Hamilton;Kathryn Morphet .SUPERCRITICAL DRYING: A NEW METHOD FOR CONSERVING WATERLOGGED ARCHAEOLOGICAL MATERIALS[J].Studies in conservation,2000(4):233-252.
[65] Stéphanie A C;Liisa M N;Néstor G G et al.Conservation of waterlogged archaeological corks using supercritical CO2 and treatment monitoring using structured-light 3D scanning[J].Journal of Supercritical Fluids,2013,79:299.
[66] 梁永煌,满瑞林,王宜飞,孙玉莲,郭萌.饱水竹木漆器的超临界CO2脱水干燥研究[J].应用化工,2011(05):839-841,843.
[67] 方北松;王宜飞;史少华.饱水竹木器超临界脱水示例[J].湖南省博物馆馆刊,2014(7):12.