采用水流分级和高能纳米冲击磨对原始SiC粉料进行微纳米粉体加工.研究结果表明:水流分级得到纯度98.42%、中位粒径0.404μm的SiC粉体,比表面积由0.8879m2/g提高到8.0321m2/g;高能冲击磨得到纯度95.5%、中位粒径0.257μm的SiC粉体,比表面积由0.8879m2/g提高到8.2773m2/g,SiC的粒径及比表面积达到半导体制造业用微纳米碳化硅粉体的技术标准.纯度分析表明碳化硅粉体的水流分级未引入杂质,化学成分基本不变;SiC粉体冲击磨加工纯度下降,其他杂质含量偏高.粉体形貌分析表明原始SiC粉料形貌为非球形,粒度分布不均匀,水流分级和冲击磨加工碳化硅粉体形貌为非球形,粒度分布较加工前更均匀.

参考文献

[1] K. SUZUKI;N. KAGEYAMA;T. KANNO.Improvement in the oxidation resistance of liquid-phase-sintered silicon carbide with aluminum oxide additions[J].Ceramics International,20056(6):879-882.
[2] Guerfi K;Lagerge S;Meziani MJ;Nedellec Y;Chauveteau G.Influence of the oxidation on the surface properties of silicon carbide[J].Thermochimica Acta: An International Journal Concerned with the Broader Aspects of Thermochemistry and Its Applications to Chemical Problems,20051/2(1/2):140-149.
[3] Marinkovic Stanojevic, Z.;Brankovi?, Z.;Jagli?i?, Z.;Jagodi?, M.;Man?i?, L.;Bernik, S.;Re?nik, A.;Brankovi?, G..Structural and magnetic properties of nanocrystalline bismuth manganite obtained by mechanochemical synthesis[J].Journal of nanoparticle research: An interdisciplinary forum for nanoscale science and technology,20118(8):3431-3439.
[4] 王宁峰;铁生年.半导体制造用碳化硅粉末加工研究[J].矿山机械,2007(10):45-47.
[5] R. Huang;H. Gu;J. Zhang.Effect of Y_2O_3-Al_2O_3-ratio on rater-granular phases and films in tape-casting alpha-SiC with high toughness[J].Acta materialia,20058(8):2521-2529.
[6] Shuqiang Ding;Sumin Zhu;Yuping Zeng.Effect of Y_2O_3 addition on the properties of reaction-bonded porous SiC ceramics[J].CERAMICS INTERNATIONAL,20064(4):461-466.
[7] 崔晓英.SiC半导体材料和工艺的发展状况[J].电子产品可靠性与环境试验,2007(04):58-62.
[8] 陈启董;郭文利;戚利强.高速气流冲击法制备陶瓷-金属复合粉体[J].中国粉体技术,2015(1):77-81.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%