采用循环伏安法(Cv)在含草酸、苯胺单体的溶液中以AZ91镁合金为基底沉积聚苯胺(Pani)涂层,并通过IR和SEM等手段对涂层的结构和形貌特征进行表征;同时通过极化曲线、开路电位-时间曲线及电化学阻抗谱(EIS)等评价涂层在3.5%NaCl溶液中的耐蚀性.结果表明,聚苯胺涂层有效提高了镁合金基体的自腐蚀电位,并导致镁合金腐蚀电流密度下降近两个数量级;长期浸泡过程中发现涂层能够有效抑制腐蚀溶液的渗透,阻止基体合金的腐蚀.

参考文献

[1] Andreia Romeiro;Carla Gouveia-Caridade;Christopher M.A. Brett.Polyphenazine films as inhibitors of copper corrosion[J].Journal of Electroanalytical Chemistry: An International Journal Devoted to All Aspects of Electrode Kinetics, Interfacial Structure, Properties of Electrolytes, Colloid and Biological Electrochemistry,2013:282-288.
[2] 徐国荣,易清风,周光喜,任凤莲.铝基体上电沉积聚苯胺膜及其耐蚀性[J].中国腐蚀与防护学报,2008(01):11-15.
[3] 张颖君,冯涛,邵亚薇,孟国哲,张涛,王福会.聚苯胺/环氧涂层对AZ91D镁合金耐蚀性能的影响[J].中国腐蚀与防护学报,2010(04):283-287,294.
[4] Guo XW.;Jiang YF.;Zhai CQ.;Lu C.;Ding WJ. .Preparation of even polyaniline film on magnesium alloy by pulse potentiostatic method[J].Synthetic Metals,2003(1/3):169-170.
[5] 蒋永锋,包晔峰,杨顺贞,高莹,田松亚.镁合金表面聚苯胺膜层防腐性能的研究[J].表面技术,2006(06):19-21.
[6] Xu-Yuan Peng;Feng Luan;Xiao-Xia Liu;Dermot Diamond;King-Tong Lau .pH-controlled morphological structure of polyaniline during electrochemical deposition[J].Electrochimica Acta,2009(26):6172-6177.
[7] 张清华,王献红,景遐斌.聚苯胺的合成及其光谱特性[J].化学世界,2001(05):242-244.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%