采用浸渍法制备了纳米晶ZSM-5负载的磷钨酸复合固体催化剂,纳米晶ZSM-5上单独负载磷钨酸时,Keggin结构磷钨酸转变为Dawson结构多酸化合物,结合镍盐后Keggin结构保持不变.以有机硫化物氧化脱硫为探针反应的研究结果表明,在低温(40℃)反应条件下,含二苯并噻吩有机硫组分的正辛烷模拟油品的脱硫率高达94.5%.

参考文献

[1] Omwoma, Solomon;Gore, Christopher T.;Ji, Yuanchun;Hu, Changwen;Song, Yu-Fei.Environmentally benign polyoxometalate materials[J].Coordination chemistry reviews,2015Mar.(Mar.):17-29.
[2] Can Li;Zongxuan Jiang;Jinbo Gao;Yongxing Yang;Fuping Tian;Fuxia Sun;Xiuping Sun;Pinliang Ying;Shaojun Wang;Chongren Han.Ultra-Deep Desulfurization of Diesel:Oxidation with a Recoverable Catalyst Assembled in Emulsion[J].Chemistry: A European journal,20049(9):2277-2280.
[3] Chen LD;Wang XS;Guo XW;Guo HC;Liu H;Chen YY.In situ nanocrystalline HZSM-5 zeolites encaged heteropoly acid H3PMo12O40 and Ni catalyst for hydroconversion of n-octane[J].Chemical Engineering Science,200716(16):4469-4478.
[4] 姜春杰;孙胜男;王旭阳;王祥生;郭洪臣;郭新闻;陈立东.甲醇脱水制二甲醚的杂多酸/纳米HZSM-5复合固体酸催化剂[J].化学学报,2013(5):810-814.
[5] 王旭阳;宋鹏月;王祥生;郭新闻;郭洪臣;杨晓宇;陈立东;姜春杰.多酸基深度加氢脱硫催化剂的原位表征和反应性能[J].应用化学,2014(8):990-992.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%