针对酸轧IF软钢切边合格率低的情况,研究了导致酸轧切边缺陷的要素和预防措施,并研究了切边剪的切边原理。通过对上线前刀具的间隙和重叠量偏差的限定,提高刀具硬度,合理搭配剪切间隙和重叠量,保持稳定高速的切边速度等措施,使IF软钢切边合格率得到极大地提高,为生产符合宽度公差要求的产品奠定了基础,并保证了轧机的顺利轧制和下道产线的稳定顺行。

Aiming at the low percent of pass of side trimming of IF steel after pickling and cold rolling, the essential fac-tors that caused the defects of side trimming and the precautionary measures were investigated and the operational princi-ple of side trimmer was researched. The measures such as limiting the side clearance and the overlapping deviation of the side trimmer before it works, increasing the hardness of the side trimmer, reasonable matchup of the side clearance and the overlapping, and keeping the stable and high speed of side trimming were taken. All the above measures increased the per-cent of pass of side trimming greatly, which laid the foundation of producing the rolled steel within width allowance and al-so ensured the smooth operation of rolling mill and stable production.

参考文献

[1] 杨必祥,侯中勇,陈志康,朱勤农.冷轧板带边部剪切质量的控制与研究[J].冶金设备,2008(05):49-51,20.
[2] 王畅,于洋,王林,陈瑾,徐海卫.含磷高强IF钢拉矫断带的原因及机制[J].钢铁,2014(05):81-87.
[3] 冯平.酸洗工序IF钢切边不良原因及对策[J].四川冶金,2002(04):11-12,7.
[4] 李文翼.冷轧板带切边浪形的成因分析和改进途径[J].宝钢技术,2004(04):1-3,6.
[5] 张蒙.圆盘剪力能参数的计算方法与选择[J].冶金设备,2010(z1):1-3,13.
[6] 孔繁华;杨大中;杨富伟 .切边圆盘剪的力能参数计算[J].一重技术,1999,82(04):15.
[7] 王永强,孙清泉,董凯,亓兴超.圆盘剪间隙调整及切边质量改进[J].山东冶金,2007(03):71-72.
[8] 马瑞杰,艾晶,郑祥臣.圆盘剪剪切原理的探讨及剪刃崩刀的分析[J].冶金设备,2012(01):43-46.
[9] 黄生银,甄圣明.冷轧圆盘剪切边过程中常见问题处理[J].江苏冶金,2008(06):62-63.
[10] 吴志生,尚继东,袁长泽.冷轧板带切边变形过程及其影响因素[J].轻合金加工技术,2001(12):23-24,31.
[11] 王刚,李广,焦兴贵.1300圆盘剪切机的设计与参数选择[J].轻合金加工技术,2001(09):20-23,36.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%