介绍了Better 117C有机硅浸渍树脂的基本性能和结构试验情况,并将其与进口树脂进行全面对比.结果表明:Better 117C有机硅浸渍树脂的各项基本性能与进口H62C树脂相当,模拟线棒和模卡的各项电性能都达到YJ90A1牵引电机的使用要求,浸渍Better 117C的YJ90A1电机定子绕组温升比浸渍H62C的低12.4~13.4℃.Better 117C有机硅浸渍树脂具有优异的电气性能、耐热性能和耐水性,适用于大功率牵引电机线圈和绕组的绝缘处理.

The basic performance and structural testing of Better 117C silicone impregnating resin were introduced, and then was compared with imported resin. The results show that the basic performance of Better 117C silicone impregnating resin is similar to the imported H62C resin. The electrical performance of the simulation winding bar and mockup can reach the requirements of YJ90A1 traction motor. The Better 117C silicone impregnating resin has excellent electrical properties, heat resistance, and water resistance, which can be used to insulation treatment of high-power traction motor coil and winding.

参考文献

[1] 陈红生.C级3551有机硅无溶剂浸渍树脂及其在牵引电机上的应用[J].电力机车与城轨车辆,2006(05):38-40,56.
[2] 余卫斌.电力机车牵引电机绝缘系统的引进及国产化[J].电力机车与城轨车辆,2007(03):1-3,7.
[3] 陈宗旻;华玮;叶学淳.C级无溶剂有机硅树脂性能及应用[J].上海大中型电机,2002(3):33-36.
[4] 李宏;何少波;夏宇.JF-9962 VPI浸渍树脂性能研究[J].电机与控制应用,2013(11):59-61.
[5] 夏宇;李翠翠;王文.JF-9960C级无溶剂浸渍树脂研制与性能研究[J].电机与控制应用,2011(5):51-54.
[6] 左瑞霖;梁国正;常鹏善;杜超云;贾艺红.耐高温无溶剂绝缘浸渍漆的研究进展[J].绝缘材料,2002(2):26-33.
[7] 衷敬和;姜其斌;黎勇;陈红生;李强军;李钦.有机硅绝缘浸渍漆的现状及发展趋势[J].绝缘材料,2008(6):21-24.
[8] 衷敬和;姜其斌;黎勇;陈红生;李强军;蔡彬芬.C级无溶剂有机硅浸渍漆的应用工艺研究[J].绝缘材料,2008(4):11-13.
[9] 周光红;姜其斌;李鸿岩;李钦;衷敬和;黎勇;李强军.国产无溶剂有机硅浸渍漆TJ 1173与进口漆的性能比较[J].绝缘材料,2010(1):42-44.
[10] 蒋大伟;姜其斌;刘跃军.加成型有机硅树脂的合成及其浸渍漆配比性能研究[J].绝缘材料,2010(2):13-16.