以固态热塑性酚醛树脂为基体,乌洛托品为固化剂,研究了乌洛托品添加量对注射型酚醛模塑料性能的影响.结果表明:当乌洛托品添加量为9%时,酚醛模塑料可以正常注射成型,成型件表面平整光亮,色泽均匀,综合性能优良.
The solid thermoplastic phenolic resin was used as matrix resin and the methenamine was used as curing agent in the preparation of injection type phenolic molding compound, and the effect of methenamine content on the properties of the injection type phenolic molding compound was studied. The results show that when the methenamine content is 9%, the phenolic molding compound could mold by injection normally, the appearance of molding product is smooth, the color is uniform, and the compre-hensive performance are good.
参考文献
[1] | 潘建光;任敏峰.注射型酚醛模塑料发展概况[J].绝缘材料通讯,2000(6):19-22. |
[2] | 孙同甲;范宏;谭军;李伯耿.剑麻纤维增强酚醛模塑料的性能[J].高分子材料科学与工程,2009(7):45-48. |
[3] | 蒋耿杰;钟立松;陈武荣;覃家波;刘建文;唐志.硅烷偶联剂对注射型酚醛模塑料的影响研究[J].绝缘材料,2014(2):33-35,40. |
[4] | 银贵晨.无氨耐燃烧酚醛注射塑料的研制[J].绝缘材料,2002(03):14-16,19. |
[5] | 范宏;周大鹏;卜志扬;李伯耿;沈培林.高外观热稳定性酚醛注塑料的研制[J].中国塑料,2004(7):61-63. |
[6] | 王玉明;徐君;潘贻芳;袁章福.偶联剂与固化剂对煤矸石改性酚醛树脂制热固性塑料的影响[J].过程工程学报,2006(2):331-333. |
[7] | 刘征.酚醛模塑料耐湿性能的改善[J].电动工具,2007(03):8-10. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%