为研究高压直流输电线路复合绝缘子的积污规律,建立了±660kV输电线路复合绝缘子流体力学模型,研究了绝缘子表面污秽撞击率及其积污特性,并进行为期一年的自然积污试验,对比试验数据与仿真结果.结果表明:绝缘子串积污规律呈现两端高中间低的趋势,绝缘子两端积污较为严重;绝缘子串两端下表面的积污比上表面严重,而绝缘子串中间部分上表面的积污比下表面严重;试验结果与仿真结果一致.

In order to study the pollution accumulation characteristic of composite insulators on the HVDC transmission line, the fluid mechanics models of composite insulators on the ±660 kV transmission line were established. The particle collision rate and pollution accumulation characteristic of the compos-ite insulators were studied. The natural contamination test lasting for one year was carried out in order to contrast the experimental data and simulation results. The results show that the both ends of the com-posite insulator string have more serious contamination than that of the middle part. For the both ends of composite insulator string, the bottom surface of the composite insulator has more serious contamina-tion than that of the top surface, and for the middle part of composite insulator string, the top surface of composite insulator has more serious contamination than that of the bottom surface. The simulation results are consistent with the experimental test results.

参考文献

[1] 邢岩;叶建亚;田文君;徐向军;王健.兰州地区110 kV线路不同伞裙结构复合绝缘子的耐污闪性能分析[J].绝缘材料,2014(3):26-29.
[2] 周瑜;李军;张仲秋;吴童生;李志玮.不同盐密灰密对瓷绝缘子污秽闪络特性影响的研究[J].绝缘材料,2009(6):58-60.
[3] 李志玮;周瑜;姚欢;冯亦佳.水泥污秽对复合绝缘子污秽闪络特性的影响研究[J].绝缘材料,2009(5):45-47,51.
[4] 王少华;胡文堂;龚坚刚;潘杰;许杨勇;刘浩军.浙江电网架空输电线路绝缘子串的自然积污特性[J].高电压技术,2014(4):1002-1009.
[5] 张锐;黄道春;吴光亚;袁田.交流特高压支柱瓷绝缘子的自然积污特性研究[J].电网技术,2014(11):3225-3231.
[6] 蒋兴良;李海波.计算流体力学在绝缘子积污特性分析中的应用[J].高电压技术,2010(2):329-334.
[7] 毕晓甜;任昂;沈庆河;刘辉;李清泉.±660 kV银东线绝缘子串的自然积污特性研究[J].绝缘材料,2015(10):45-49,54.
[8] 温作铭 .基于流体力学的覆冰地区用复合绝缘子伞裙结构研究[D].重庆大学,2007.
[9] 王彬;梁曦东;张轶博;罗兵;李震宇;刘瑛岩;周远翔.交、直流电压下复合绝缘子和瓷绝缘子的自然积污试验[J].高电压技术,2009(9):2322-2328.
[10] 彭功茂;关志成;张福增;梅红伟;王黎明.复合绝缘子的直流人工污秽试验方法[J].高电压技术,2011(3):570-576.
[11] 李恒真;赖江宇;雷乾;邓诗雨;刘刚;李立浧.污秽颗粒在绝缘表面的碰撞和吸附[J].高电压技术,2012(10):2596-2603.
[12] 王晶;陈林华;刘宇;梁曦东.电场对复合绝缘子积污特性影响的探究[J].高电压技术,2011(3):585-593.
[13] 梁飞;MacAlpine Mark;关志成;张若兵.污秽绝缘子表面干区形成的影响因素[J].高电压技术,2012(10):2604-2610.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%