应用不确定性纹理谱进行金属断口形貌的识别;采用最小距离分类器,对等轴韧窝、拉长韧窝、解理、疲劳和沿晶等典型断口进行分类.分析结果表明,这种方法具有较好的分类效果.

参考文献

[1] Zhang D. Practical Analysis of Machinery Failure. Beijing: National Defense Press, 1997:24(张栋.机械失效的实用分析.北京:国防工业出版社,1997:24)
[2] Komai K, Minoshima K, Ishii S. JSME. Inter J (A). 1993,3(2): 220
[3] Yan Y H, Wang D J, Huang Y H, Wang Q H, Wang T B.Acta Metall Sin, 1997, 33:386(颜云辉,王德俊,黄雨华,王清昊,王彤波.金属学报,1997,33:386)
[4] Yan Y H, Gao J H, Liu Y, Cao Y G, Lei S C. Acta MetalSin, 2002, 38:309(颜云辉,高金鹤,刘勇,曹宇光,雷世超.金属学报,2002,38:309)
[5] Ye Y F,Zhang Z.J Mater Eng,2003,(4):44(叶宇飞,张峥.材料工程,2003,(4):44)
[6] Lee Y G, Lee J H, Hsueh Y C. Neurocomputing, 1998, 20:115
[7] Lee Y G, Lee J H, Hsueh Y C. Electron Lett, 1995, 31(12):959
[8] Ramze Rezaee M, Goedhart B, Lelieveldt B P E. Pattern Recognition, 1999, 32:2011
[9] Li S Y. Fuzzy Control. Neurocontrol and Intelligent Cybernetics. Harbin: Harbin Institute of Techonology Press,1998:35(李士勇.模糊控制·神经控制和智能控制论.哈尔滨:哈尔滨工业大学出版社,1998:35)
[10] Bian Z Q,Zhang X G. Pattern Recognition.Beijing:Tsinghua University Press,1999:186(边肇祺,张学工.模式识别.北京:清华大学出版社,1999:186)
[11] American Socity For Metals ed,translated by Deng R H.Metals Handbook(8th Edition,Vol.9).Beijing:China Machine Press.1985:52,76(美国金属学会著,邓日红译.金属手册(第八版,第九卷).北京:机械工业出版社,1985:52,76)
[12] Engel L,Klingele H eds,translated by Meng X M.An Atlas of Metal Damage.Beijing:China Machine Press,1990:32,36,79(Engel L,Klingele H著,孟锡明译.金属损伤图谱(下).北京:机械工业出版社,1990:32,36,79)
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%