利用液态硅为原料,以碳和二氧化硅粉末组成的混合物作为催化剂,通过液态硅与一氧化碳之间的气-液相碳热反应,一步合成了高纯度的碳化硅微细粉体,制得的碳化硅粉体的平均颗粒尺寸为D50=0.41um.利用XRD,SEM,激光粒度分析和元素分析对粉体进行了表征,并讨论了碳化硅粉体的形成机理.
参考文献
[1] | Friedrich Schroder.Gmelin Handbook of Inorganic Chemistry,8th edition,Berlin:Springer-Verlag,1986.178-185. |
[2] | Michael B.Bever.Encyclopedia of Materials Science and Engineering,vol 6.New York:Pergamon Press,1986.4403-4408. |
[3] | 时利良,赵宏生,闫迎辉,等.材料导报,2006,20(6):239-242. |
[4] | 陈立富(CHEN Li-Fu).无机材料学报(Journal of Inorganic Materials),1994,9(4):465-470. |
[5] | Martin H P,Ecke R,Muller E.J.Euro.Ceram.Soc.,1998,18:1737-1742. |
[6] | 潘顺龙,杨岩峰,张敬杰,等(PAN Shun-Long,et al).无机材料学报(Journal of Inorganic Materials),2006,21(6):1319-1324. |
[7] | Henry N.Baumann Jr.J.Electrochemical Soc.,1963,110(4):298-306. |
[8] | Kuhn W E.J.Electrochemical Soc.,1963,110 (4):298-306. |
[9] | 黄希祜.钢铁冶金原理,第1版.北京:冶金工业出版社,1981.295-300. |
[10] | Okada K,Kato H,Nakajima K.J.Am.Ceram.Soc.,1994,77 (6):1691-1693. |
[11] | Kennedy P,North B.Proc.Br.Ceram.Soc.,1983,33:1-15. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%