采用柠檬酸盐前驱体技术,合成了粒径约为20~70 nm的尖晶石结构MnFe2O4纳米颗粒,用聚乙烯亚胺(PEI)对MnFe2O4纳米颗粒进行表面处理后,以异丙醇钛为前驱物,采用sol-gel法在纳米MnFe2O4表面包覆锐钛矿型TiO2纳米层形成核壳结构.利用透射电子显微镜(TEM)、X射线衍射仪(XRD)和振动样品磁强计等测试手段对样品的结构、形貌、粒径以及磁学性能等进行了表征.采用罗丹明B的光催化降解反应对所制催化剂的活性进行了评价.结果表明,核壳结构TiO2/MnFe2O4复合纳米颗粒的光催化活性随着壳层厚度的增加而增强,当达到一定厚度以后,其催化活性不随壳层厚度的增加而改变.复合颗粒中TiO2含量达到30 wt%,反应时间4 h时,TiO2/MnFe2O4磁性光催化剂对罗丹明B的光降解率达到100%,与纯TiO2纳米粉体的催化活性相当,且光催化活性稳定,是一种便于回收、可重复使用的高效光催化剂.

参考文献

[1] Mayya K S,Gittins D I,Caruso F.Gold-titania core-shell nanoparticles by polyelectrolyte complexation with a titania precursor[J].Chem Mater,2001,13:3833-3836.
[2] Teng F,Tian Z J,Xiong G X,Xu Z S.Preparation of CdS-SiO2 core-shell particles and hollow SiO2 spheres ranging from nanometers to microns in the nonionic reverse microemulsions[J].Catalysis Today,2004,95:93-95.
[3] 孙聆东,付雪峰,钱程,等.水热法合成CdS/ZnO核壳结构纳米微粒[J].高等学校化学学报,2001,22(6):879-882.Sun Lingdong,Fu Xuefeng,Qian Cheng,et al.Synthesis of core/shell structural CdS/ZnO nanoparticles by hydrothermal method[J].Chemical Journal of Chinese Universities,2001,22(6):879-882.
[4] Ocana M,Hsu W P,Matijevic E.Preparation and properties of uniform-coated colloidal particles 6:Titania on zinc oxide[J].Langmuir,1991,7:2911-2916.
[5] 张敬畅,李青,曹维良.超临界流动干燥法TiO2/Fe2O3和TiO2/Fe2O3/SiO2复合纳米粒子及光催化性能[J].复合材料学报,2005,22(1):79-81.Zhang Jingchang,Li Qing,Cao Weiliang.Preparation and photocatalytic properties of TiO2/Fe2O3 and TiO2/Fe2O3/SiO2 nano-composite photocatalyst by supercritical fluid drying[J].Acta Materiae Compositae Sinica,2005,22(1):79-81.
[6] 余家国,赵修建,赵青南.掺锡TiO2复合薄膜的制备和光催化性能的研究[J].复合材料学报,2001,18(1):79-82.Yu Jiaguo,Zhao Xiujian,Zhao Qingnan.Preparation of Sn-doped TiO2 composite thin films by sol-gel processing and their photo-catalytic properties[J].Acta Materiae Compositae Sinica,2001,18(1):79-82.
[7] Fujishima A,Rao T N,Truk D A.Titanium dioxide photocatalysis[J].J Photochem Photobiol C:Photochem Rev,2000,1:1-21.
[8] Modestov A D,Lev O.Photocatalytic oxidation of 2,4-dichlorophenoxyacetic acid with titania photocatalyst:Comparison of supported and suspended TiO2[J].J Photochem Photobiol A:Chem,1998,112:261-270.
[9] Wang R,Hashimoto K,Fujishima A,et al.Photogeneration of highly amphiphilic TiO2 surfaces[J].Adv Mater,1998,10:135-138.
[10] 朱永法,李巍,何俣,等.不锈钢金属丝网上TiO2纳米薄膜光催化剂的研究[J].高等学校化学学报,2003,24(3):465-468.Zhu Yongfa,Li Wei,He Yu,et al.Studies on nanometer TiO2 film photocatalyst supported on stainless steel wire gauze[J].Chemical Journal of Chinese Universities,2003,24(3):465-468.
[11] Yuan R,Fu X,Wang X,et al.Template synthesis of hollow metal oxide fibers with hierarchical architecture[J].Chem Mater,2006,19:4700-4705.
[12] 王秀宇,杨桂琴,严乐美,等.纳米晶MnFe2O4的低温共沉淀法合成及表征[J].化学研究与应用,2004,16(1):115-116.Wang Xiuyu,Yang Guiqin,Yan Lemei,et al.Preparation of MnFe2O4 nanocrystals by coprecipitation at low temperature and their characterization[J].Chemical Research and Application,2004,16(1):115-116.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%