通过三维编织炭纤维增强碳化硅基复合材料(3D C/SiC)在各种氧化气氛中的环境实验,研究了氧化气氛中材料的质量变化率和剩余强度随温度变化规律及其相关性.根据3D C/SiC复合材料各组元的作用,对其微观组织及炭纤维预制体的氧化损伤演变进行了分析.结果表明,在各个氧化温度区间内,3D C/SiC质量变化率与剩余强度随温度变化的规律基本相同,两者结果相互对应.对于3D C/SiC,用质量变化率作为对环境损伤敏感性表征的一个基本指标,比用剩余强度表征更科学可靠.

参考文献

[1] Jamet J F,Lamicq P.Composite thermostructures:An overview of the French experience[C]// Naslain R,Lamon J,Doumeingts D,eds.High Temperature Ceramic Matrix Composites.Bordeaux:Woodhead Publishing Limited,1993:735-742.
[2] Christin F.Design,fabrication,and application of thermostructural composites (TSC) like C/C,C/SiC,and SiC/SiC composites[J].Advanced Engineering Materials,2002,4(12):903-912.
[3] Naslain R.Design,preparation and properties of non-oxide CMCs for application in engines and nuclear reactors:An overview[J].Composites Science and Technology,2004,64 (2):155-170.
[4] Lamouroux F,Camus G,Thébault J.Kinetics and mechanisms of oxidation of 2D woven C/SiC composites Ⅰ:Experimental approach[J].Journal of the American Ceramic Society,1994,27(8):2049-2057.
[5] Lamouroux F,Bourrat X,Naslain R,et al.Structure/oxidation behavior relationship in the carbonaceous constituents of 2D-C/PyC/SiC composites[J].Carbon,1993,31(8):1273-1288.
[6] Lamouroux F,Camus G.Oxidation effects on the mechanical properties of 2D woven C/SiC composites[J].Journal of the European Ceramic Society,1994,14(2):177-188.
[7] Cheng Laifei,Xu Yongdong,Zhang Litong,et al.Oxidation behavior from room temperature to 1500 degrees C of 3D-C/SiC composites with different coatings[J].Journal of the American Ceramic Society,2002,85(4):989-991.
[8] 尹洪峰.LPCVI-C/SiC复合材料结构与性能的研究[D].西安:西北工业大学,2000.Yin Hongfeng.Research of microstructure and properties of LPCVI-C/SiC composites[D].Xi'an:Northwestern Polytechnical University,2000.
[9] Xu Y,Zhang L,Cheng L,et al.Three-dimensional carbon/silicon carbide composites prepared by chemical vapor infiltration[J].Journal of the American Ceramic Society,1997,80(7):1897-1900.
[10] 李建章.航空发动机热端部件模拟环境下3D C/SiC的微结构演变与失效机制[D].西安:西北工业大学,2006.Li Jianzhang.Microstructural evolving and failure mechanism of 3D C/SiC in environment simulating hot-section component service in aero-engine[D].Xi'an:Northwestern Polytechnical University,2000.
[11] 殷小玮.3DC/SiC复合材料的环境氧化行为[D].西安:西北工业大学,2001.Yin Xiaowei.Oxidation behaviors of 3D C/SiC composites in oxidizing environments[D].Xi'an:Northwestern Polytechnical University,2000.
[12] Cheng L F,Xu Y D,Zhang L T,et al.Factorization method for failure mechanism analysis of C/C and C/SiC composites[J].Science and engineering of composite Materials,2002,10(1):45-49.
[13] Lovell D R.Carbon and high performance fibres directory and databook[M].6th edition.London:Chapman & Hall,1995:viii.
[14] Yamada K,Mohri M.Properties and applications of silicon carbide ceramics[M]// Shigeyuki Somiya,Yoshizo Inomata,eds.Silicon Carbide Ceramics-1,Fundamental and Solid Reaction.London:Elsevier Applied Science,1991:13-44.
[15] Hirai T,Sasaki M.Silicon carbide prepared by chemical vapor deposition[M]// Shigeyuki Somiya,Yoshizo Inomata,eds.Silicon Carbide Ceramics-1,Fundamental and Solid Reaction.London:Elsevier Applied Science,1991:77-98.
[16] 杜善义,王彪.复合材料细观力学[M].北京:科学出版社,1998.Du Shanyi,Wang Biao.Mesomechanics of composites[M].Beijing:Science Press,1998.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%