目前商用快速成型机的制备工艺参数与原料都受到限制,不易制作骨骼模型,为克服上述缺点,使用自行开发的快速成型机制作骨骼模型.本研究主要是以羟基磷灰石、二氧化硅溶胶和少许分散剂混合之浆料为原料,经由适当的调整加工参数后,可成型生物陶瓷生胚.生胚试片分别在1200℃、1300℃、1400℃烧结,并对其体积收缩率、表面粗糙度和抗压强度进行分析.经由培养MG63类骨母细胞,研究骨骼模型表面的细胞活性.结果显示,生胚在1200℃烧结时性能较佳,抗压强度明显上升,表面粗糙度Ra为12.04 μm,较适合MG63类骨母細胞生长.

参考文献

[1] Eshraghi S,Das S.Mechanical and microstructure properties of polycaprolactone scaffolds with one-dimensional,two-dimensional,and three-dimensional orthogonally oriented porous architectures produced by selective laser sintering.Acta Biomaterialia.,2010 (6):2467-2479.
[2] 李武松.颅颜整形手术用植入物之设计与制作.桃园:国立中央大学硕士论文,1990.
[3] Peng R S,Wang J B,Yao Q Z.Application study of rapid prototyping manufacturing in media.Chinese Journal of Lasers,2005,29(3):87-88.
[4] CUI Zhi-Zhong,LI Di-Chen,QIAO Guan-Jun,et al.Peparation of porous carbon template with controllable channels by phenolic resin pyrolyzing.Journal of Inorganic Materials,2006,21(4):848-854.
[5] Liu F H,Liao Y S.Fabrication of inner complex ceramic parts by selective laser gelling.Journal of the European Ceramic Society.,2010(30):3283-3289.
[6] Liu F H.Manufacturing porous multi-channel ceramics by laser gelling Ceramics International,2011 (37):2789-2794.
[7] 赵震锦,张翀,张扬,等.表面粗糙度对种植体钛片表面成骨细胞的影响.解剖科学进展,2008,14(2):178-182.
[8] Goergiou G,Knowles J C.Glass reinforced hydroxyapatite for hard tissue surgery.Biomaterials,2001(22):2811-2815.
[9] Ruys A J,Wei M,Sorrell C C,et al.Sintering effect on the strength of hydroxyapatite.Biomaterials,1995,16(5):409-415.
[10] ZHANG Lei-Lei,LI He-Jun,LI Ke-Zhi,et al.Effect of surface roughness of carbon/carbon composites on osteoblasts.Journal of Inorganic Materials,2008,23(2):341-345.
[11] Ponsonnet L,Comte V,Othmane A,et al.Effect of surface topography and chemistry on adhesion,orientation and growth of fibroblasts on nickel-titanium substrates.Materials Science and Engineering C.,2002,21(1/2):157-165.
[12] Montanaro L,Arciola C R,Campoccia D,et al.In vitro effects on MG63 osteoblast-like cells following contact with two roughnessdiffering fluorohydroxyapatite-coated titanium alloys.Biomaterials,2002(23):3651-3659.
[13] 范震,贾爽,苏剑生,等种植体表面粗糙度对成骨细胞增殖及ALP含量的影响.口腔颌面外科杂志,2009,19(2):128-131.
[14] Rosa A L,Beloti M M.Rat bone marrow cell response to titanium and titanium alloy with different surface roughness.Clin Oral Implants Res.,2002(14):43-48.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%