采用浸渍法制备了一系列不同Cu含量的Cu-ZSM-5催化剂,并用于NH3选择性催化还原(SCR)NO反应.结果表明,当Cu含量为8%时,Cu-ZSM-5催化剂的活性最高;当空速为30 000h-1,在198~440℃反应时NO转化率均高于80%,最高可达97%,且空速的影响较小经快速水热老化后,该催化剂活性明显优于商用V基催化剂.H2O和SO_2对Cu-ZSM-5催化剂的SCR活性有所影响,但可明显恢复.X射线衍射和NH_3程序升温脱附结果表明,当Cu-ZSM-5中Cu含量为8%时,进入ZSM-5中阳离子位的Cu较多,催化剂的活性较高,且其表面具有较多的酸中心和酸量,从而有利于SCR反应.

参考文献

[1] Br6cr S;Hammer T .[J].7p1 Catal B,2000,28:101.
[2] Garcia-Bordeje E;Calvillo L;Lazaro M J;Moliner R .[J].Applied Catalysis B:Environmental,2004,50:235.
[3] Ka?par J;Fornasiero P;Hickey N .[J].Catalysis Today,2003,77:419.
[4] Adams K M;Cavataio J V;Hammerle R H .[J].Applied Catalysis B:Environmental,1996,10:157.
[5] Carja G;Kameshima Y;Okada K;Madhusoodana C D .[J].Applied Catalysis B:Environmental,2007,73:60.
[6] van Kooten W E J;Liang B;Krijnsen H C;Oudshoorn O L Calis H P A van den Bleek C M .[J].Applied Catalysis B:Environmental,1999,21:203.
[7] Sjǒ6vall H;Olsson L;Fridell E;Blint R J .[J].Applied Catalysis B:Environmental,2006,64:180.
[8] Krishna K;Makkee M .[J].Catalysis Today,2006,114:23.
[9] Rivallan M;Berlier Q;Ricchiardi G;Zecchina A Nechit M T Olsbye U .[J].Applied Catalysis B:Environmental,2008,84:204.
[10] Qi G S;Wang Y H;Yang R T .[J].Catalysis Letters,2008,121:111.
[11] Richter M;Trunschke A;Bentrup U;Brzezinka K W Schreier E Schneider M Pohl M M Fricke R .[J].Journal of Catalysis,2002,206:98.
[12] Qi G S;Yang R T;Chang R .[J].Catalysis Letters,2003,87:67.
[13] Komvokis V G;Iliopoulou E F;Vasalos I A;Triantafyllidis K S Marshall C L .[J].Applied Catalysis A:General,2007,325:345.
[14] Li L D;Zhang F X;Guan N J;Richter M Fricke R .[J].Catalysis Communications,2007,8:583.
[15] Sullivan J A;Cunningham J .[J].Applied Catalysis B:Environmental,1998,15:275.
[16] Ganemi B;Bjǒ6mbom E;Demirel B;Paul J .[J].Microporou sMesoporous Mater,2000,38:287.
[17] Pironc R;Ciambelli P;Moretti G;Russo G .[J].Applied Catalysis B:Environmental,1996,8:197.
[18] Ma A Z;Muhler M;Griinert W .[J].Chemical Engineering and Technology,2000,23:273.
[19] Lang R T;Yang R T .[J].Journal of Catalysis,2000,194:80.
[20] Qi GS.;Yang RT. .Low-temperature selective catalytic reduction of NO with NH3 over iron and manganese oxides supported on titania[J].Applied Catalysis, B. Environmental: An International Journal Devoted to Catalytic Science and Its Applications,2003(3):217-225.
[21] Pieterse JAZ;Pirngruber GD;van Bokhoven JA;Booneveld S .Hydrothermal stability of Fe-ZSM-5 and Fe-BEA prepared by wet ion-exchange for N2O decomposition[J].Applied Catalysis, B. Environmental: An International Journal Devoted to Catalytic Science and Its Applications,2007(1/2):16-22.
[22] Blasco T;Corma A;Martinez-Triguero J .[J].Journal of Catalysis,2006,237:267.
[23] Cavataio G;Jen H W;Warner J R;Girard J W,Kim J Y,Lambert C K .SAE Paper,2008-01-1025[R].
[24] Sierraalta A;Bermudez A;Rosa-Brussin M .Density functional study of the interaction of Cu+ ion-exchanged zeolites with H2O and SO2 molecules[J].Journal of molecular catalysis, A. Chemical,2005(1/2):203-210.
[25] 唐晓龙,郝吉明,徐文国,李俊华.新型MnOx催化剂用于低温NH3选择性催化还原NOx[J].催化学报,2006(10):843-848.
[26] Qi G S;Yang R T;Chang R .[J].Applied Catalysis B:Environmental,2004,51:93.
[27] de Oliveira M L M;Silva C M;Moreno-Tost R;Farias T L,Jimenez-Lódpez A,Rodíriguez-Castelól6n E .[J].Applied Catalysis,2009,88:420.
[28] Lí Z J;Flytzani-Stephanopoulos M .[J].Applied Catalysis B:Environmental,1999,22:35.
[29] Machida M;Uto M;Kurogi D;Kijima T .[J].Chemistry of Materials,2000,12:3158.
[30] Sullivan J A;Cunningham J;Morris M A;Keneavey K .[J].Applied Catalysis B:Environmental,1995,7:137.
[31] Roy S;Hegde M S;Madras G .[J].Applied Energy,2009,86:2283.
[32] Sirilumpen M;Yang R T;Tharapiwattananon N .[J].Journal of Molecular Catalysis A:Chemical,1999,137:273.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%