基于PET塑料薄膜取代硬质玻璃作为基板材料制备柔性液晶盒时,采用传统制备工艺会产生盒厚度不均以及盒中残留气泡等现象,导致柔性液晶器件性能变差.采用辊压工艺可以有效地解决上述问题,文章对其工艺流程进行了详细描述.实验发现,通过在辊压工艺中加热两片基板以降低溶液的黏度,能够有效地避免气泡残留,获得厚度均匀的柔性液晶盒.应用辊压工艺和聚合物分散胆甾相液晶,成功地制备了尺寸为7 cm2的反射式柔性双稳态液晶盒.利用正交偏光显微镜观察了聚合物分散液晶的相形态,紫外分光光度计测试了其光电性能:最高反射率为22.8%,对比度为2.259,阈值电压为78 V,饱和电压为99 V.

参考文献

[1] Jang S J,Jung J W,Kim J H,et al.Pixel-isolated liquid-crystal mode by using a patterned anisotropic phase separation for flexible LCDs[J].Journal of the SID,2007,15(2):119-125.
[2] Wang Q B,Guo R,Kumar S.Method for fabrication of liquid-crystal cells with narrow gap,fast switching,and flexible plastic substrates[J].J.Soc.Inf.Display,2006,14(6):545-550.
[3] Vorflusev V,Kumar S.Phase-separated composite films for liquid crystal displays[J].Science,1999,283(19):1903-1905.
[4] Sato H,Fujikake H,Sato F,et al.A4-sized flexible ferroelectric liquid-crystal displays with micro color filters[J].Journal of SID,2005,13(6):461-468.
[5] Carter S A,LeGrange J D,Wiltzius P,et al.Dependence of the morphology of polymer dispersed liquid crystals on the UV polymerization process[J].J.Appl.Phys.,1997,81(9):5992-5999.
[6] Kato K,Tanaka K,Tsuru S,Sakai S.Color image formation using polymer-dispersed cholesteric liquid crystal[J].Jpn.J.Appl.Phys.,1993(32):4600-4604.
[7] Huang Y P,Zhu X Y,Ren H W,et al.Full-color transflective cholesteric LCD with image-enhanced reflector[J].J.Soc.Inf.Display,2004,12(4):417-422.
[8] 刘国柱,黄子强,杨文君,等.低阈值电压聚合物分散性液晶膜的电光特性[J].液晶与显示,2009,24(3):383-388.
[9] 王丽萍,许锐,黄顺刚,等.添加液晶对PDLC膜电-光性能参数的影响[J].液晶与显示,2010,25(4):554-557.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%