酸雨是对石材造成化学腐蚀的最重要因素之一.考察了pH值为4.0的模拟酸雨对两种石材有机氟硅防护材料(Pelicoat和Mellerud)的影响.实验结果发现随着腐蚀的进行,两种防护材料的疏水性降低,防护效果下降.SEM电镜发现用防护材料处理过的样品经过模拟酸雨8 h腐蚀后,试样表面出现大量网状孔洞.

参考文献

[1] 王晓蓉.环境化学[M].南京:南京大学出版社,1993
[2] 孙崇基.酸雨[M].北京:中国环境科学出版社,2001
[3] 聂王焰,周艺峰.石刻保护有机硅涂料的研究[J].涂料工业,2005(08):16-18.
[4] P.Cardiano;R.C.Ponterio;S.Sergi;S.Lo Schiavo;P.Piraino .Epoxy-silica polymers as stone conservation materials[J].Polymer: The International Journal for the Science and Technology of Polymers,2005(6):1857-1864.
[5] TONILO L;POLl T;CASTELVETRO V.Tmloring new fluorinated acrylic copolymers as protective coatings for marble[J].Journal of Cultural Heritage,2002(03):309-316.
[6] 冯增昭.沉积岩石学[M].北京:石油工业出版社,1993
[7] 徐飞高,汤剑,高士祥.南京市麒麟镇麒麟石刻风化壳的表征[J].环境化学,2008(02):251-255.
[8] Okochi H.;Hasegawa S.;Saito N.;Kubota K.;Igawa M.;Kameda H. .Deterioration of concrete structures by acid deposition - an assessment of the role of rainwater on deterioration by laboratory and field exposure experiments using mortar specimens[J].Atmospheric environment,2000(18):2937-2945.
[9] IDKAMNT.laboratory experiments of the investigation of the effects of sulphuric acid on the deterioration of carbonate stones and surface corrosion[J].Water,Air & Soil Pollution,1999(114):1-12.
[10] H BRAVO A;R SOTO A.Effect of acid rain on building material of the Tajin arehaeological zone in Veracmz,Mexico[J].Environmental Pollution,2006(144):655-660.
[11] TONIOLO L;POLI T;CASTELVETRO V.Tailoring new fluorinated acrylic copolymers as protective coatings for marble[J].Journal of Cultural Heritage,2002(03):309-316.
[12] COULSON S R;WOODWARD I;BADYAL J P S.Superrepellent composite fluoropolymer surfaces[J].Journal of Physical Chemistry B,2000(104):8836-8840.
[13] 霍润科 .酸性环境下砂浆砂岩材料的受酸腐蚀过程及其基本特性劣化规律的试验[D].西安:西安理工大学,2006.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%