以Sr2+, Y3+和Eu3+的混合硝酸盐溶液为阳离子溶液, 以(NH4)2CO3为沉淀剂, 共沉淀法制备了碳酸盐前驱体, TG-DSC分析结果表明, 随着(NH4)2CO3浓度的升高, 前驱体组成由碱式碳酸盐向正盐转变. 以CS2为硫化剂, 高温煅烧前驱体合成了SrY2S4:Eu2+红色荧光粉. XRD表明前驱体经800 ℃处理得到纯相SrY2S4. 荧光光谱和SEM研究表明在[Sr(NO3)2+Eu(NO3)3]:[Y(NO3)3]:[(NH4)2CO3]=0.25:0.50:2.00(摩尔比)条件下制备前驱体, 然后1050 ℃煅烧4 h所得荧光粉的发光强度最大, 粒径小于1 μm, 粒子形貌呈椭球. Eu2+在SrY2S4基质中的最佳掺杂摩尔分数是0.6%.

参考文献

[1] Schevciw O;White W B .The optical absorption edge of rare earth sesquisulfides and alkaline earth-rare earth sulfides[J].Materials Research Bulletin,1983,18(09):1059.
[2] Yuta M M;White W B .Photoluminescence of sulfide phosphors with the MB2S4 composition[J].Journal of the Electrochemical Society,1992,139(08):2347.
[3] 廉世勋,李承志,毛向辉,张华京.CaS∶Eu绿转红功能的农用研究[J].稀土,2002(03):37-40.
[4] Lowema CK.;Smith TE.;Vanderah TA. .THE TERNARY YTTRIUM SULFIDES, CAY2S4, SRY2S4, AND BAY2S4 - STRUCTURES AND PROPERTIES[J].International Journal of Quantum Chemistry,1995(2):363-372.
[5] Purdy AP.;George CF.;Berry AD. .SYNTHESIS, STRUCTURE, AND THIOLYSIS REACTIONS OF PYRIDINE SOLUBLE ALKALINE EARTH AND YTTRIUM THIOLATES[J].Inorganic Chemistry: A Research Journal that Includes Bioinorganic, Catalytic, Organometallic, Solid-State, and Synthetic Chemistry and Reaction Dynamics,1997(15):3370-3375.
[6] Hu YS;Zhuang WD;Ye HQ;Zhang SS;Fang Y;Huang XW .Preparation and luminescent properties of (Ca1-xSr,)S : Eu2+ red-emitting phosphor for white LED[J].Journal of Luminescence: An Interdisciplinary Journal of Research on Excited State Processes in Condensed Matter,2005(3):139-145.
[7] Tokunaga S;Mikami A .Effects of Zn-doping on red-luminescence in Eu-doped (Mg,Ca)S phosphor films[J].Applied Surface Science: A Journal Devoted to the Properties of Interfaces in Relation to the Synthesis and Behaviour of Materials,2005(1/4):533-536.
[8] Liya Zhou;Jianxin Shi;Menglian Gong .Preparation of SrR_2O_4:Eu~(3+) (R=Y, Lu) phosphor and its photoluminescence properties[J].Materials Letters,2005(16):2079-2084.
[9] Zhou Liya;Shi Jianxin;Gong Menglian .Red phosphor SrY2O4∶Eu3+ synthesized by the sol-gel method[J].Journal of Luminescence,2005,11(3-4):285.
[10] 闻雷,孙旭东.碳酸盐前驱物制备Y2O3超细粉及透明陶瓷[J].中国稀土学报,2003(02):166-169.
[11] Tsai M S;Hon M H.The effects of sulphurizing agent on the formation of calcium lanthanum sulphide[J].Materials Science and Engineering,1994(B26):29.
[12] Tsai MS.;Hon MH.;Wang LH. .FORMATION OF CALCIUM LANTHANUM SULFIDE BY CARBONATE COPRECIPITATION AND CS2 SULFURIZATION[J].Journal of the American Ceramic Society,1995(5):1185-1190.
[13] Tsay B J;Wang L H;Hon M H .Formation and densification of Pb0.1Ca0.9La2S4 powders by sulfidization of modified metal alkoxides[J].Ceramics International,1999,25:303.
[14] Tsay BJ.;Hon MH.;Wang LH. .Formation and densification of CaLa2S4 powders by sulfidization of modified metal alkoxides in different atmospheres[J].Materials Science & Engineering, B. Solid-State Materials for Advanced Technology,2000(1):31-35.
[15] 武汉大学;吉林大学.无机化学[M].北京:高等教育出版社,1983:269.
[16] 北京师范大学;华中师范大学;南京师范大学无机教研室.无机化学[M].北京:人民教育出版社,1981:985.
[17] 王少成,胡建国,马林,张小庆,王惠琴,徐燕.尿素水解法合成细粒径高亮度Y2O3∶Eu红色荧光粉[J].复旦学报(自然科学版),2003(06):1015-1019.
[18] 易宪武;黄春辉;王慰.钪稀土元素(无机化学丛书)[M].北京:科学出版社,1998:228.
[19] 徐剑,张剑辉,张新民,郭崇峰,苏锵.Ga2S3∶Eu2+和SrGa2+xS4+y∶Eu2+系列荧光粉的发光性能研究[J].中国稀土学报,2003(06):635-638.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%