采用光学显微镜和TEM观察等方法,分析了ZE42镁合金热挤压板材在不同退火温度和时间条件下的显微组织结构.结果表明:该合金板材经过退火热处理后均发生明显的再结晶组织转变,晶粒尺寸在10 ~60μm之间,合金基体中存在大量含有稀土元素的第二相颗粒,这些第二相在热变形过程中破碎成细小的颗粒,促进了再结晶晶粒的形核.当退火温度一定时,随着保温时间的延长,该合金板材的平均晶粒尺寸首先增加,随后少量减小,最后又随退火时间的增加而增加;当保温时间一定时,随着退火温度的增加,晶粒平均尺寸持续增加,并且温度越高,增长速率越大.同时,通过晶粒长大动力学分析和计算建立了该合金再结晶晶粒长大的动力学模型,通过计算可知:该合金的再结晶晶界迁移激活能为15.32 kJ·mol-1.

参考文献

[1] A.A. Luo;R.K. Mishra;A.K. Sachdev .High-ductility magnesium-zinc-cerium extrusion alloys[J].Scripta materialia,2011(5):410-413.
[2] YU WenBin,CHEN ZhiQian,CHENG NanPu,GAN BingTai,HE Hong,LI XueLian,HU JinZhu.High-strength wrought magnesium alloy with dense nano-scale spherical precipitate[J].科学通报(英文版),2007(13):1867-1871.
[3] WANG Zhongjun,XU Yang,WANG Zhaojing,CHENG Jia,KANG Baohua,ZHU Jing.Solidification behavior, microstructure and tensile properties of ZK60-Er magnesium alloys[J].稀土学报(英文版),2011(06):558-561.
[4] J.D. Robson;D.T. Henry;B. Davis .Particle effects on recrystallization in magnesium-manganese alloys: Particle-stimulated nucleation[J].Acta materialia,2009(9):2739-2747.
[5] Mendis C;Ohishi K;Kawamura Y;Honma T,Kamado S,Hono K .Precipitation-hardenable Mg-2.4Zn-0.1Ag-0.1Ca-0.16Zr(at.%)wrought magnesium alloy[J].Acta Materialia,2009,57(03):749.
[6] Anbu S;Ramanathan S .A comparaive study of the wear behavior of as-cast and hot extruded ZE41A magnesium alloy[J].Journal of Alloys and Compounds,2010,502(02):495.
[7] 何兰强,马鸣龙,李兴刚,李永军,张奎.Mg-9.0Y-3.0MM-0.6Zr合金均匀化热处理研究[J].稀有金属,2011(02):164-169.
[8] Wang Z J;Zhu J;Cheng J .Effects of rare earth and Ca elements additions on the microstructure and tensile properties of Mg6 Zn-3 Al-1 Cu alloys[J].Advanced Science Letters,2011,4(11):3691.
[9] D.H. Bae;S.H. Kim;D.H Kim .Deformation behavior of Mg-Zn-Y alloys reinforced by icosahedral quasicrystalline particles[J].Acta materialia,2002(9):2343-2356.
[10] Wang Z J;Yang Q X;Qiao J .Phase structure of ZK660-1Er magnesium alloy compressed at 450 ℃[J].Transactions of Nonferrous Metals Society of China,2010,20(S):567.
[11] Wang Z J;Jia W P;Cui J Z .Study on the deformation behavior of Mg-23.6 wt.% Er magnesium alloy[J].Journal of Rare Earth~,2007,25(06):44.
[12] Wang Z J;Zhang C B;Shao X H;Cui J Z,Le Q C .Effect of erbium on microstructure and thermal compressing flow behavior of Mg-6Zn-0.5Zr alloy[J].Transactions of Norferrous Metals Society of China,2006,12(S):1774.
[13] Li, L.;Zhang, X. .Hot compression deformation behavior and processing parameters of a cast Mg-Gd-Y-Zr alloy[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2011(3):1396-1401.
[14] Yi Sangbong;Bohlen Jan;Heinemana Frank;Letzig Dietmar .Mechanical anisotropy and deep drawing behavior of AZ31 and ZE10 magnesium alloy sheets[J].Acta Materialia,2010,58(02):592.
[15] 彭伟平,刘腾,何良菊,李培杰,曾攀.中间退火对镁合金板材组织和性能的影响[J].材料热处理学报,2007(03):58-62.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%