以Li2CO3、Mn(NO3)2和M(NO3)3(M=La,Nd,Y)为原材料,用溶胶-凝胶方法和微波加热技术合成了纳米级尖晶石LiMxMn2O4(M=La,Nd,Y)材料,XRD实验表明, 微波合成的材料相纯度较高,充放电实验表明,在LiMn2O4中掺杂摩尔比为0.006的La 、Nd和Y可以提高其电化学比容量和充放电循环性能.
参考文献
[1] | Zhong Q M,Bonakdarpour A,Zhang M J. J Electrochem Soc, 1997,144:205 |
[2] | Jun Sugiyama,Taroh Aosumi,Tatsumi Hioki, et al. J Power Sources,1997,68:641 |
[3] | Pistoia G,Rosati R. J Power Sources,1996,58:135 |
[4] | Thackeray M M,Mansuetto M F,Bates J B. J Power Sources,1997, 68:153 |
[5] | Sato K,Poojary D M,Clearfild A. J Solid State Chemistry,1997,131:84 |
[6] | 藤岛昭,相泽益男,井上 (日)著(Auth). 陈震(CHEN Zhen),姚建年(YAO Jian -Nian)译(Trans). 电化学测定方法(Methods of The Electrochemcal Measrement). 北京 (Beijing):北京大学出版社(Beijing University Press),1995:325 |
[7] | Feng L,Chang Y Q,Wu L, et al. J Power Sources,1996,63:149 |
[8] | Liu Z L,Yu Aishui,Lee J Y. J Power Sources,1998,74 :228 |
[9] | Jang D H,Shin Y J,Seung M O. J Electrochem Soc,1996,143(7):2204 |
[10] | Xia Yongyao,Zhou Yunhong,Masaki Yoshio. J Electrochem Soc,1997,144(8):2593 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%