用核磁共振(NMR)技术研究了国产的和拜耳公司生产的2种溶聚丁苯的组成及其链化学结构. 结果表明,这2种溶聚丁苯具有十分相近的共聚物组成(其中苯乙烯单元的摩尔分数均约为14.0%). 国产溶聚丁苯中反式1,4-丁二烯含量较高(trans-1,4摩尔分数为49.7%),而拜耳公司的溶聚丁苯具有很高的顺式1,4结构含量(摩尔分数为49.4%),形成了顺式1,4-丁二烯嵌段,并且乙烯基含量也明显少于国产丁苯胶. 这种结构导致拜耳丁苯胶具有低的玻璃化转变温度,并与天然橡胶有很好的相容性.
参考文献
[1] | Moore D G,Day G L. Elastomerics[J],1985,3:22 |
[2] | Day G L,Futamura S. Kautsch Gummi Kunstst[J],1987,40(1):39 |
[3] | Schuring D J. Rubber Chem Tech[J],1995,68:600 |
[4] | Takino K,Nakayama R,Yamada Y, et al. Rubber Chem Tech[J],1997,70:584 |
[5] | Manley K,Barry M. Tire Technology International[M]. Dorking:UK & International Press,1998:72 |
[6] | CHEN Shi-Zhao(陈士朝). J Synth Rubber Ind(合成橡胶工业)[J],1997,20:6 |
[7] | MA De-Zhu(马德柱),HAO Wen-Tao(郝文涛),XU Wen-Zong(徐文总), et al. Acta Polym Sin(高分子学报)[J],2001,2:153 |
[8] | XU Wen-Zong(徐文总),LIANG Li(梁俐),MA De-Zhu(马德柱). Tire Ind(轮胎工业)[J],2001,2:91 |
[9] | XU Wen-Zong(徐文总),HAO Wen-Tao(郝文涛),MA De-Zhu(马德柱). Chin J Appl Chem(应用化学)[J],2001,18(1):44 |
[10] | Sardelist K,Michels H J,Allen G. Polymer[J],1984,25:1 011 |
[11] | Katritzky A R,Weiss D E. J Chem Soc Chem Commun[J],1974,10:401 |
[12] | Sarkar M D,De P P,Bhowmick A K. Polymer[J],2000,41:907 |
[13] | Van der Velden G,Didden C,Veermans T, et al. Macromolecules[J],1987,20:1 252 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%