由于陶瓷属于脆性材料,在机加工过程中易引入微裂纹等非本征缺陷和残余应力等机加工缺陷,从而造成材料损伤.通过改善陶瓷材料的显微结构,可设计和研制出有可加工性的陶瓷材料.对玻璃陶瓷、Ti3SiC2、Si3N4、SiC及氧化物陶瓷等多种可加工陶瓷材料进行了简单介绍.

参考文献

[1] 贾志新,艾冬梅,张勤河,张建华.工程陶瓷材料加工技术现状[J].机械工程材料,2000(01):2-4,16.
[2] Padture N P .In situ-toughened silicon carbide[J].Journal of the American Ceramic Society,1994,77(02):519-523.
[3] Frei H;Granthwohl G .Microstructure and strength of advanced ceramics after machining[J].Ceramics International,1993,19:93-104.
[4] Johnson W D;Evans A G;Marshall D B et al.Residual stresses in machined ceramic surfaces[J].Journal of the American Ceramic Society,1986,69(01):44-47.
[5] 高玲,赵世坤,杜大明,李华平,杨海涛.磨加工及残余应力对氮化硅陶瓷强度的影响[J].山东陶瓷,2003(04):12-15.
[6] 张航 .热处理对热压陶瓷复合材料机械加工损伤的影响[J].机械工程材料,1998,22(01):14-15,47.
[7] 张航;龚江宏;杨正方 .ZTM陶瓷表面机加工损伤的初步研究[J].陶瓷学报,1997,18(01):23-26.
[8] Tomoko Uno;Toshihiro Kasuga;Nakayama Shin .Preparation of high-strength calcium-mica-containing machinable glassceramics[J].Journal of the Ceramic Society of Japan,1992,100(05):703-707.
[9] 秦小梅,孙祥云.可切削玻璃陶瓷的透明玻璃形成及云母析晶[J].东北大学学报(自然科学版),2000(06):656-658.
[10] 马新沛,李光新,沈莲,金志浩.一种新型云母玻璃陶瓷的切削行为与显微结构[J].无机材料学报,2004(01):48-52.
[11] Barsoum MW.;Elraghy T. .SYNTHESIS AND CHARACTERIZATION OF A REMARKABLE CERAMIC - TI3SIC2[J].Journal of the American Ceramic Society,1996(7):1953-1956.
[12] Elraghy T.;Barsoum MW.;Kalidindi SR.;Zavaliangos A. .DAMAGE MECHANISMS AROUND HARDNESS INDENTATIONS IN TI3SIC2[J].Journal of the American Ceramic Society,1997(2):513-516.
[13] Y.W.Bao,Y.C.Zhou.MECHANICAL PROPERTIES OF Ti3SiC2 AT HIGH TEMPERATURE[J].金属学报(英文版),2004(04):465-470.
[14] Kawai C;Yamakawa A .Effect of porosity and microstructure on the strength of SisN4:designed microstructure for high strength,high thermal shock resistance and facile machining[J].Journal of the American Ceramic Society,1997,80(10):2705-2708.
[15] Taira M;Yamaki M .Ranking machinability of nine machinable ceramics by dental high-speed cutting tests[J].Journal of Materials Science Letters,1994,13(07):480-482.
[16] Padture NP.;Xu HHK.;Lawn BR.;Evans CJ. .ENHANCED MACHINABILITY OF SILICON CARBIDE VIA MICROSTRUCTURAL DESIGN[J].Journal of the American Ceramic Society,1995(1):215-217.
[17] Suresh Baskaran;John W Halloran .Fibrous monolithic ceramics:Ⅱ,flexural strength and fracture behavior of silicon crabide/graphite system[J].Journal of the American Ceramic Society,1993,76(09):2217-2224.
[18] Kuo D H;Kriven W M .Mechanical behavior and microtructure of SiC and SiC/TiB2 ceramics[J].Journal of the European Ceramic Society,1998,18(01):51-57.
[19] 李永利,乔冠军,金志浩.可加工性BN/Al2O3陶瓷基复合材料的制备[J].中国有色金属学报,2002(06):1179-1183.
[20] 邱世鹏,刘家臣,刘志锋,葛志平,于爱兵,李鸿祥.CePO4/Ce-ZrO2可加工陶瓷加工机理的研究[J].硅酸盐学报,2003(04):341-345.
[21] Davis JB.;Housley RM.;Morgan PED.;Marshall DB. .Machinable ceramics containing rare-earth phosphates[J].Journal of the American Ceramic Society,1998(8):2169-2175.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%