在醇水混合体系中以乙醇为溶剂,六次甲基四胺(HMT)为缓释沉淀剂采用均匀沉淀法制备了纳米CeO2粉体,用透射电子显微镜(TEM)、X射线衍射仪(XRD)等方法对纳米颗粒进行了表征,研究了醇水比、反应温度、反应时间对纳米颗粒粒径的影响.结果表明:随着乙醇含量的增加,纳米颗粒粒径逐渐减小,随着反应温度的升高和反应时间的延长,纳米颗粒粒径增大.
参考文献
[1] | 陈建清 .超细二氧化铈制备及其化学机械抛光机理研究[D].江苏大学,2004. |
[2] | Hu MZC.;Byers CH.;Payzant EA. .Sol-gel and ultrafine particle formation via dielectric tuning of inorganic salt-alcohol-water solutions[J].Journal of Colloid and Interface Science,2000(1):20-36. |
[3] | Fang CS.;Chen YW. .Preparation of titania particles by thermal hydrolysis of TiCl4 in n-propanol solution[J].Materials Chemistry and Physics,2003(3):739-745. |
[4] | CHEN Pei-lin;CHEN 1-wei .Reactive cerium (Ⅳ) oxide powders by the homogeneous precipitation method[J].Journal of the American Ceramic Society,1993,76(06):15-83. |
[5] | 李霞章,陈志刚,陈建清,陈杨.醇水均匀沉淀法制备纳米CeO2粉体工艺及机理研究[J].机械工程材料,2006(03):68-70. |
[6] | Chen HI;Chang HY .Homogeneous precipitation of cerium dioxide nanoparticles in alcohol/water mixed solvents[J].Colloids and Surfaces, A. Physicochemical and Engineering Aspects,2004(1/3):61-69. |