采用中频感应提拉法生长了Yb:FAP晶体.对晶体生长中影响晶体质量的因素特别是原料的处理、CaF2的挥发等进行了研究和讨论.运用ICP-AES测定Yb3+离子在Yb:FAP晶体中的分凝系数.对Yb:FAP晶体进行了高分辨X射线的四圆衍射实验,结果表明晶体具有比较高的晶格完整性.
参考文献
[1] | Klbas M R;Anderson N G;Laidig W D et al.Strained-layer InGaAs-GaAs-AlGaAs Photopumped and Current Injection Laser[J].IEEE Journal of Oceanic Engineering,1998,24:1605. |
[2] | Giesen A;Huger H;Voss A et al.Scalable Concept for Diode-pumped High-power Solid-state Lasers[J].Applied Physics B-Lasers and Optics,1994,58:365. |
[3] | Payne S A;Deloach L D;Smith L K et al.Ytterbium-doped Apatite-structure Crystals.A New Class of Laser Materials[J].Journal of Applied Physics,1994,76(01):497. |
[4] | DeLoach L D;Payne S A;Kway W L et al.Vibrational Structure in the Emission Spectra of Yb3+-doped Apatite Crystals[J].Journal of Luminescence,1994,62:85. |
[5] | Naray-Szabo S .The Structure of Apatite Ca5(PO4)3F[J].Zeitschrift für Kristallographie,1930,75:387. |
[6] | Roth R S;Wegas T;Cook L P.Phase Diagrams for Ceramists[M].The American Ceramic Society Inc,1983:213. |
[7] | 杨培志,邓佩珍,柴耀,徐军,陈伟,王浩炳.掺镱氟磷酸钙(Yb∶FAP)晶体的生长[J].硅酸盐学报,1999(02):219-223. |