在四辊冷轧试验机和Gleeble-1500试验机上进行了热轧微碳钢板的冷轧和退火试验.用D/max-RC衍射仪测量了试样的1/4层织构,并用Roe软件进行了ODF分析.研究表明,所研究的热轧微碳深冲板压下率约为75%,退火升温速度为20~40℃/h时,试样为{111}织构特征;压下率较大(80%)时,退火织构为较弱的{111}组分.无论{111}织构还是非{111}织构都是在形核阶段开始形成,在晶粒长大优先长大,受到定向形核和选择生长双重机制的作用.
参考文献
[1] | Sanak Mishra;C Darmann .Role and control of texture in deepdrawing steels[J].International Metals Reviews,1982,27(06):307-320. |
[2] | 何崇智,张志军,田德新,刘浩.武钢微碳深冲钢板的织构特征与成型性[J].钢铁,1998(07):0. |
[3] | 吕庆功,陈光南,常军,程兴德,唐历,周家琮.微碳深冲钢板的非{111}织构特征及其对-γ,△γ值的影响[J].金属学报,2001(06):567-570. |
[4] | Yasunobu NAGATAKI;Yoshihiro HOSOYA .Origin of the Recrystallization Texture Formation in an Interstitial Free Steel[J].ISIJ International,1996(4):451-460. |
[5] | T Urabe;J. J. Jonas .Modeling Texutre Change during the Recrystallization of an IF Steel[J].ISIJ International,1994,34(05) |
[6] | W B Hutchinson .Recrystallisation Textures in Iron Resulting from Nucleation at Grain Boundaries[J].Acta Metallurgy,1989,37(04):1047-1056. |
[7] | Christian Klinkenberg;Dierk Raabe;Kurt Lucke .Influenceof volume fraction and dispersion rate of grain-boundary cementite on the cold-rolling textures of low- carbon steel[J].Steel Research International,1992,63(06):262-269. |