为了提高钛合金(Ti6A14V)表面化学镀镍层与基体的结合强度,对其镀前活化工艺(浸锌活化)进行了改进和优化,并用电化学测试技术探讨了活化时间对活化过程的影响,结果表明,在本文提出的活化工艺条件下,经过二次浸锌能保证镀层与钛合金基体间良好的结合强度.
参考文献
[1] | 彭艳萍.军用新材料的应用现状及发展趋势(待续)[J].材料导报,2000(01):13-16. |
[2] | Demasi-Marein J T;Gupta D K .Protective coatings in the gas turbine en gine[J].Surface and Coatings Technology,1994,70(01):68. |
[3] | Mallory G O .The relationship between stress and adhesion of electroless nickel-phosphorus deposits on zincated aluminum[J].Plating and Surface Finishing,1985,72(06):86. |
[4] | Critchlow G W;Brewis D W .Review of surface pretreaments for titanium alloys[J].International Journal of Adhesion and Adhesives,1995,15(03):161. |
[5] | Sharma A K;Bhojaraj H .Electroless nickel and gold plating on titanium alloys for space applications[J].Metal Finishing,1992,90(07):23. |