以硫酸钴为主盐,酒石酸钠为配位剂,硼氢化钠为还原剂,采用改进的逐步滴加还原剂的方式控制反应进程,用化学镀法制备了Co-B合金包覆羰基铁颗粒的复合粉体.用正交设计方法确定了镀液组成和工艺参数:18 g/L CoSO4·7H2O,60 g/L酒石酸钠,1 g/L NaBH4,铁粉装载量2 g/L,温度75℃,pH值>13,并进一步讨论了各因素对镀速的影响,对镀覆后的复合粉体的结构、成分进行了表征.结果表明,通过优化镀覆工艺,可以获得包覆均匀的复合粒子.
参考文献
[1] | 罗永弟.超细羰基铁发展、市场及应用前景[J].四川冶金,2001(03):39-42. |
[2] | 邢丽英.隐身材料[M].北京:化学工业出版社,2004 |
[3] | Abicht H P;Vohzkc D;Scannich H .Preparation characterization and sintering behavior of barium titanate powders coated with Ba-,Ca -,Si-and Ti-containing components[J].Materials Chemistry and Physics,1997,51:35-41. |
[4] | Armstrong T R;Buchanan R C .Influence of core-shell on the internal stress state and permittivity response of zirconate -modified barium titanate[J].Journal of the American Ceramic Society,1990,73(05):1268-1276. |
[5] | Viltzke D;Gablenz S;Abicht H P et al.Surface modification of barium titanate powder particles[J].Materials Chemistry and Physics,1999,61:110-116. |
[6] | 赵心怡,叶明泉,韩爱军.无机超细粒子表面改性技术研究进展[J].塑料工业,2006(z1):16-19. |
[7] | C.D. Iacovangelo .Continuous In-Situ Regeneration of Electroless Nickel Baths During Powder Plating[J].Plating & Surface Finishing,1995(9):77-82. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%