以辊棒废料为主要原料,在CaO-MgO-SiO2-Al2O3体系中,研究烧结温度、保温时间、成型方式和压力大小对中铝瓷球显微结构及性能的影响规律及其机理.结果表明:在150MPa等静压成型,1330oC烧结,保温3h的工艺条件下,研制含铝量小于60%的中铝瓷球的性能最优异,磨损率为0.0503%/h,密度为3.1062g/cm3,与市售90瓷球相比,磨损率与之持平,白度与市售90瓷球不相上下.
参考文献
[1] | Dogan C.P.;Hawk J.A. .Role of composition and microstructure in the abrasive wear of high-alumina ceramics[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,1999(2):1050-1058. |
[2] | Esposito L;Tucci A .Microstructural dependence of friction and wear behavious in low purity alumina ceramic[J].Wear,1997,205:88-96. |
[3] | M. Sathiyakumar;F. D. Gnanam .Influence of additives on density, microstructure and mechanical properties of alumina[J].Journal of Materials Processing Technology,2003(3):282-286. |
[4] | Medvedovski E .Wear- resistant engineering ceramic[J].Wear,2001,249:821-828. |
[5] | 秦麟卿,吴伯麟,谢济仁,段兴龙.耐磨氧化铝研磨球的生产和应用[J].武汉理工大学学报,2001(03):12-14,18. |
[6] | 秦麟卿,吴伯麟,谢济仁,宋京红,段兴龙,牟善彬.微孔对氧化铝瓷球磨损特性的影响[J].武汉工业大学学报,2000(05):12-14. |
[7] | Mukhopadhag AK .Grain size effect on abrasive wear mechanisms in alumina ceramics[J].Wear,1993,162-164:258-268. |
[8] | Krell A.;Klaffke D. .EFFECTS OF GRAIN SIZE AND HUMIDITY ON FRETTING WEAR IN FINE-GRAINED ALUMINA, AL2O3/TIC, AND ZIRCONIA[J].Journal of the American Ceramic Society,1996(5):1139-1146. |
[9] | Kwon S;Gary L .Sintering of mixture of seeded boehmite and ultrafine α- alumina[J].Journal of the American Ceramic Society,2000,83:83-88. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%