应用SEM研究了磷酸四钙(TTCP)和无水磷酸氢钙(DCPA)组成的磷酸钙骨水泥(CPC)体系水化过程中浆体的微结构.结果表明:完全硬化的CPC由纳米级针状羟基磷灰石微晶组成,微晶与人体骨有类似的低结晶度和结构特性.CPC产物结晶形态与Ca与P摩尔比有关,Ca与P摩尔比减小,CPC水化产物的轴比增大而形态较细长.
参考文献
[1] | Brown W E;Chow L C .Dental restorative cement paste[P].US:4518430,1985-05-21. |
[2] | Constantz BR;Ison IC;Fulmer MT;Poser RD;Smith ST;Vanwagoner M .SKELETAL REPAIR BY IN SITU FORMATION OF THE MINERAL PHASE OF BONE[J].Science,1995(5205):1796-1799. |
[3] | Costantino P D;Friedman C D;Jones K et al.Experimental hydroxyapatite cement cranioplasty[J].Plastic and Reconstructive Surgery,1992,90(02):3174-185. |
[4] | Brown W E;Chow L C.A new calcium phosphate, water-setting cement[A].Westerville Ohio:American Ceramic Society,1986:352-379. |
[5] | Fulmer M J;Brown P W .The kinetics of hydroxyapatite formation at low temperature[J].Journal of the American Ceramic Society,1991,74(05):934-940. |
[6] | Bonfield W .Composites for bone replacement[J].Journal of Biomedical Engineering,1988,10:522-526. |
[7] | Elliot J C.Structure and Chemistry of the Apatites and other Calcium Orthophosphates[M].Amsterdam:Elsevier Science,1994 |
[8] | Yubao L;Klein C P .Shape chang and phase transition of needle like non-stoimetric appatite crystals[J].Journal of Materials Science:Materials in Medicine,1994,5(05):263-267. |