采用溶胶-凝胶法制备了Ca3Co4O9粉,确定了适用于Ca3Co4O9粉制备的方法及工艺条件,并利用XRD、SEM 等方法分析表征样品.实验结果表明,以乙二醇为溶剂,柠檬酸为螯合剂,加入添加剂制得凝胶,干凝胶在750~900 ℃下烧结2 h,制得了20~30 nm的片状单晶Ca3Co4O9粉.