脱脂是陶瓷注射成型工艺的制约性步骤.通过热分析的方法研究了PW+EVA+SA的热特性.通过计算的方法和实测的方法得到粘结剂整体的热失重曲线,发现两者较为接近,继而提出了一个定量评价粘结剂脱脂特性的物理参量--脱脂惯量.通过对脱脂惯量的计算发现PW78%+EVA21%+SA1%粘结剂体系具有最好的脱脂特性.

参考文献

[1] Trunec M;Cihlar J .Removal of thermoplastic binders from ceramic green bodies[J].Ceramics-Silikaty,1997,41:67-80.
[2] Zhang J G;Edirisinghe M J;Evans J R G .A catalogue of ceramic injection moulding defects and their causes[J].Industrial Ceramics,1989,9:72-82.
[3] Chartier T.;Baumard JF.;Ferrato M. .SUPERCRITICAL DEBINDING OF INJECTION MOLDED CERAMICS[J].Journal of the American Ceramic Society,1995(7):1787-1792.
[4] Ebenhoch J;Ter Maat J.Ceramic injection molding with a polyacetal based binder system[A].Princenton:Metal Powder Industries Federation,1993:73-89.
[5] Tsai D S;Chen W W .Solvent debinding kinetics of alumina green bodies by powder injection molding[J].Ceramics International,1995,21:257-264.
[6] Mutsuddy B C;Ford R G.Ceramic Injection molding[M].London:Chapman and Hall,1995:66-128.
[7] Shaw H M;Edirisinghe M J .Removal of binder from ceramic bodies fabricated using plastic forming methods[J].American Ceramic Bulletin,1993,72:94-99.
[8] Hrdina KE.;Oliveira A.;Kaviany M.;Halloran JW. .Chemistry of removal of ethylene vinyl acetate binders[J].Journal of Materials Science,1998(11):2795-2803.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%