经正交试验确定了三价铬电镀黑铬的最佳镀液组成和工艺条件,并对优选的三价铬镀液及镀层进行性能测试,结果表明:镀液的分散能力约为15%;镀液的覆盖能力约为95%;还测定了几种镀液的阴极极化曲线,并进行了比较,最优镀液的阴极极化曲线的极化度最大.电镀5 min的镀层厚度约为0.5 μm,镀层的主要组分为Cr、O、Co、P和Na.

参考文献

[1] 屠振密;杨哲龙;张景双 等.三价铬电镀黑铬新工艺研究[J].防腐包装,1987,5(03):27-29.
[2] M.R. Bayati;M.H. Shariat;K. Janghorban .Design of chemical composition and optimum working conditions for trivalent black chromium electroplating bath used for solar thermal collectors[J].Renewable energy,2005(14):2163-2178.
[3] M.El-Sharif .Replacing hexavalent chromium in electroplating[J].Transactions of the Institute of Metal Finishing,1997(6):B143-B147.
[4] 屠振密.三价铬镀铬的国内外研究和发展[J].哈尔滨工业大学学报,1980(01):109-121.
[5] Anandan C.;Grips VKW.;Rajam KS.;Jayaram V.;Bera P. .Investigation of surface composition of electrodeposited black chrome coatings by X-ray photoelectron spectroscopy[J].Applied Surface Science: A Journal Devoted to the Properties of Interfaces in Relation to the Synthesis and Behaviour of Materials,2002(1/4):254-260.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%