研究了低层错能奥氏体不锈钢和高锰钢低温下的变形行为,根据两者拉伸应力-应变曲线硬化阶段的相似性,提出曲线由基体硬化、行为软化和结构硬化三部分合成,应力-应变曲线的上凹特征是软化主导与硬化共同作用的结果.分析了两种材料变形过程的相似性与不同点及其原因.
参考文献
[1] | 张旺峰;陈瑜眉;朱金华.一种新型拉伸曲线规律研究[J].西安交通大学学报 |
[2] | G B Olson;M Azrin .Transformation behavior of TRIP steels[J].Metallurgical and Materials Transactions,1978,9A:713-721. |
[3] | C H White;R W K Honeycombe .Structureal changes during the deformation of high-purity iron-manganese-carbon alloys[J].The Journal of the Iron and Steel Institute,1962,200:457-466. |
[4] | Y N Dastur;W C Leslie .Mechanism of work hardening in Hadfield manganese steel[J].Metallurgical and Materials Transactions,1981,12A:749-59. |
[5] | 刘军海 .[D].西安:西安交通大学,1988. |
[6] | R E Schramm;R P Reed .Stacking fault energies of seven commercial austenitic stainless steels[J].Metallurgical and Materials Transactions,1975,6A:1345-1351. |
[7] | L Remy .Kinetics of F.C.C deformation twinning and its relationship to stress-strain behavior[J].Acta Materialia,1978,26:443-451. |
[8] | 朱瑞富,吕宇鹏,李士同,张福成.高锰钢的价电子结构及其本质特性[J].科学通报,1996(14):1336-1338. |