研究了温度和活性元素Cr对Ni基高温钎料在3D-Cf/SiC陶瓷基复合材料上润湿的影响.采用扫描电镜与能谱仪检查界面微观结构与元素分布,通过X射线衍射仪检测界面产物.实验结果表明:升高温度,Ni基钎料在Cf/SiC上的润湿角减小;并且随钎料中的Cr的质量分数增加,润湿角减小.润湿过程属于反应润湿,润湿界面生成多种碳化物和硅化物.

参考文献

[1] Michael J. Verrilli;Elizabeth J. Opila;Anthony Calomino .Effect of Environment on the Stress-Rupture Behavior of a Carbon-Fiber-Reinforced Silicon Carbide Ceramic Matrix Composite[J].Journal of the American Ceramic Society,2004(8):1536-1542.
[2] Robert Schafrik;Robert Sprague .Gas turbine materials[J].Advanced Materials & Processes,2004(3):33-36.
[3] LOCATELLI M R;DALGLEISH B J;NAKASHIMA K et al.New approaches to joining ceramics for high-temperature applications[J].Ceramics International,1997,23:313-322.
[4] SUGANUMA K;MIYAMOTO Y;KOIZUMI M .Joining of ceramics and metals[J].Annual Review of Materials Science,1988,18:47-73.
[5] Lee HK.;Lee JY. .A STUDY OF THE WETTING, MICROSTRUCTURE AND BOND STRENGTH IN BRAZING SIC BY CU-X(X=TI,V,NB,CR) ALLOYS[J].Journal of Materials Science,1996(15):4133-4140.
[6] 童巧英,成来飞,张立同.二维C/SiC复合材料连接的显微结构与性能[J].材料工程,2002(11):14-16,21.
[7] 陈康华;包崇玺;刘红卫 .金属/陶瓷润湿性(上)[J].材料科学与工程,1997,15(03):6-10.
[8] Li SJ.;Zhou Y.;Duan HP. .Wettability and interfacial reaction in SiC/Ni plus Ti system[J].Journal of Materials Science,2002(12):2575-2579.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%