测试比较了国内新研和国外两种约束阻尼带的性能,结果表明:国内新研约束阻尼带剥离强度较高,但剥离后在基体上有残留胶;国外约束阻尼带损耗因子较高,阻尼功能温域较宽;随着粘贴层数的增多,国内外约束阻尼带损耗因子均增大,且最大损耗因子对应温度均向低温移动.

The constrained-layer damping tapes including the oversea and the domestic were tested and compared. The differences between the oversea and the domestic in peel strength and damping properties were discovered. The results show that the domestic constrained-layer damping tapes possess higher peel strength than that of the oversea. And the peel fracture of the domestic constrained-layer damping tape was hybrid fracture. The oversea constrained-layer damping tapes possess larger maximum loss factor and wider damping temperature range than that of the domestic tape. The loss factor of two kinds of damping tapes increases and the temperature at the maximum loss factor reduces with increasing the layers of constrained-layer damping tapes.

参考文献

[1] 张治平,张泽朋,翁建乐.聚合物阻尼材料研究进展[J].化工新型材料,2008(07):20-22,27.
[2] 张友南,杨军,贺才春,唐先贺.阻尼材料的研究与应用[J].噪声与振动控制,2006(02):38-41.
[3] 刘棣华.粘弹性阻尼材料减振降噪应用技术[M].北京:宇航出版社,1990
[4] 曾海泉,罗跃刚,杨元凤,鄢利群.高分子阻尼材料及阻尼结构[J].特种橡胶制品,2001(05):17-20.
[5] GJB 3045-1997,粘弹性阻尼材料通用规范[S].
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%