高级检索

研究了纳米0.1%(质量分数)Al颗粒对SnAgCu无铅钎料与铜基板之间界面反应的影响,研究两种无铅钎料界面在-55~125℃热循环过程中的生长行为及其焊点力学性能变化.结果表明:随着热循环次数的增加,界面层金属间化合物的厚度明显增加,焊后界面层金属间化合物为Cu6 Sns相,在热循环过程中在Cu6Sn5和Cu基板之间出现Cu3Sn 相.发现纳米Al颗粒的添加,界面层金属间化合物的厚度明显减少,纳米颗粒对界面层的生长具有明显的抑制作用.同时对焊点在热循环过程中的可靠性进行分析,发现焊点的拉伸力随着循环次数的增加逐渐降低,含纳米Al颗粒的焊点具有明显的优越性,在焊点服役期间,焊点失效路径为Cu6Sn5/Cu3Sn的界面处.

参考文献

[1] 张亮,韩继光,郭永环,何成文,张剑.含纳米铝颗粒SnAgCu钎料组织与性能[J].焊接学报,2013(06):65-68.
[2] PING LIU;PEI YAO;JIM LIU .Effect of SiC Nanoparticle Additions on Microstructure and Microhardness of Sn-Ag-Cu Solder Alloy[J].Journal of Electronic Materials,2008(6):874-879.
[3] K. Bukat;M. Koscielski;J. Sitek;M. Jakubowska;A. Mlozniak .Silver nanoparticles effect on the wettability of Sn-Ag-Cu solder pastes and solder joints microstructure on copper[J].Soldering & Surface Mount Technology,2011(3):150-160.
[4] A.S.M.A. Haseeb;M.M. Arafat;Mohd Rafie Johan.Stability of molybdenum nanoparticles in Sn-3.8Ag-0.7Cu solder during multiple reflow and their influence on interfacial intermetallic compounds[J].Materials Characterization,2012:27-35.
[5] 张亮,韩继光,郭永环,何成文,赖忠民,王宏伟.WLCSP器件Sn3.9Ag0.6Cu焊点疲劳寿命预测[J].焊接学报,2012(03):97-100.
[6] Liang Zhang;Song Bai Xue;Guang Zeng .Interface reaction between SnAgCu/SnAgCuCe solders and Cu substrate subjected to thermal cycling and isothermal aging[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,2012(1):38-45.
[7] 薛松柏,吴玉秀,崔国平,张玲.热循环对QFP焊点强度及其微观组织影响规律的数值模拟[J].焊接学报,2006(11):1-4.
[8] 刘琼,卢斌,栗慧,王娟辉,朱华伟,焦羡贺.添加0.1%Ce对Sn-3.0Ag-0.5Cu焊料与铜基板间的金属间化合物的影响[J].中国稀土学报,2007(06):707-712.
[9] 齐丽华,黄继华,张建纲,王烨.热-剪切循环条件下Sn-3.5Ag-0.5Cu/Cu(Ni)界面化合物生长行为研究[J].稀有金属材料与工程,2007(02):241-244.
[10] Asit Kumar Gain;Tama Fouzder;Y.C. Chan .Microstructure, kinetic analysis and hardness of Sn-Ag-Cu-1 wt% nano-ZrO_2 composite solder on OSP-Cu pads[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,2011(7):3319-3325.
[11] SONG J M;LIU Y R;LAI Y S et al.Influence of trace alloying elements on the ball impact test reliability[J].Microelectronics Reliability,2012,52(01):180-189.
[12] Liang Zhang;Cheng-wen He;Yong-huan Guo;Ji-guang Han;Yong-wei Zhang;Xu-yan Wang .Development of SnAg-based lead free solders in electronics packaging[J].Microelectronics and reliability,2012(3):559-578.
[13] 陈建勋,赵兴科,刘大勇,黄继华,邹旭晨.电子组装用SnAgCu系无铅钎料的研究进展[J].材料工程,2013(09):91-98.