连续氮化硅陶瓷纤维是透波/承载一体化陶瓷基复合材料的关键原材料,也是制约复合材料耐高温性能与力学性能的关键因素.系统研究了国防科技大学研制的连续氮化硅纤维的组成结构及其力学性能和介电性能,分析了纤维在氮气中高温处理后组成结构与单丝强度变化规律.结果表明,氮化硅纤维主要以Si3 N4结构存在,组成上接近化学计量比,介电常数为68,介电损耗为0.01~0.08,室温单丝强度约1.5 GPa,弹性模量140 GPa,在1350℃以下纤维强度保留率超过90%,在1400和1450℃氮气中处理1 h仍保持了非晶结构,强度保留率分别为75%和30%,综合性能满足了高温透波复合材料的基本要求.

Amorphous silicon nitride fibers were prepared by nitridation of polycarbosilane fiber,and their com-position,structure and properties were characterized using popular methods.KD-SN fiber was produced by Na-tional University of Defense Technology (NUDT),given near chemical stoichiometric composition of Si3 N4 with traces oxygen and carbon.The volume density and linear density were 2.3 g/cm3 and 280 tex respectively. The dielectric constant was 6-8 and the tanδwas 0.01-0.08.The tensile strength and modulus of elasticity were 1.5 and 140 GPa respectively.The high temperature tests were taken in the nitrogen atmosphere at 1 300, 1 350,1 400 and 1450 ℃ with a holding time of 1 h.The tensile strength was kept above 90% of the original fi-ber.Over 1 350 ℃,the tensile strength and modulus decreased sharply,even though the composition changed little.The fibers could keep their amorphous state before 1 450 ℃ but nanopores’volume was increased signifi-cantly.Overall,the KD-SN silicon nitride fiber offers a promising choice for high temperature ceramic matrix composites.

参考文献

[1] Riley F.L.;,.Silicon Nitride and Related Materials[J].Journal of the American Ceramic Society,20002(2):245-265.
[2] Hagen Klemm.Silicon Nitride for High-Temperature Applications[J].Journal of the American Ceramic Society,20106(6):1501-1522.
[3] 宋永才;冯春祥;薛金根.氮化硅纤维研究进展[J].高科技纤维与应用,2002(2):6-11.
[4] Kiyoshi Sato;Hiroki Morozumi;Osamu Funayama.Developing Interfacial Carbon-Boron-Silicon Coatings for Silicon Nitride-Fiber-Reinforced Composites for Improved Oxidation Resistance[J].Journal of the American Ceramic Society,20027(7):1815-1822.
[5] Zou, Chunrong;Zhang, Changrui;Li, Bin;Wang, Siqing;Xie, Zhengfang;Song, Yongcai.Fabrication and properties of borazine derived boron nitride matrix wave-transparent composites reinforced by 2.5 dimensional fabric of Si-N-O fibers[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2015:420-427.
[6] 兰琳;夏文丽;陈剑铭;刘玲;丁绍楠;刘安华.聚碳硅烷氮化热解法制备Si3 N4纤维[J].功能材料,2013(20):2981-2984.
[7] Yang Li;Jiacheng Gao.Preparation of silicon nitride ceramic fibers from polycarbosilane fibers by γ-ray irradiation curing[J].Materials Letters,2013Nov.1(Nov.1):102-104.
[8] 黎阳;高家诚.γ辐照聚碳硅烷先驱丝热解制备氮化硅陶瓷纤维及性能[J].硅酸盐学报,2013(10):1318-1322.
[9] Scarlett Widgeon;Gabriela Mera;Yan Gao.Effect of Precursor on Speciation and Nanostructure of SiBCN Polymer-Derived Ceramics[J].Journal of the American Ceramic Society,20135(5):1651-1659.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%