以BVRE重轨钢为研究对象,通过真空冶炼、锻造和轧制工艺制备合格的重轨钢试样.在此基础上,系统研究稀土重轨钢奥氏体晶粒的长大动力学.实验结果表明,随着加热温度的提高,稀土重轨钢奥氏体晶粒呈指数关系长大;随着保温时间的延长,稀土重轨钢奥氏体晶粒长大呈抛物线规律.重轨钢中添加微量的稀土,可以明显降低不同加热条件下的奥氏体晶粒尺寸.模型计算结果表明,重轨钢的奥氏体晶粒长大公式分别为:d4.80=d4.800+ 2.82×1028texp(- 556450/RT)(不加稀土)和d5.34=d5.340 +4.52×1032texp(- 646890/RT)(稀土重轨钢).稀土主要通过晶界的偏聚机制使奥氏体晶粒长大激活能由556450J·mol-1增加到646890J·mol-1,从而抑制奥氏体晶粒尺寸的增加.
参考文献
[1] | 林勤,郭锋,朱兴元.碳锰洁净钢中镧和铈在晶界的行为[J].中国稀土学报,2006(06):729-733. |
[2] | 邱巨峰.稀土在晶界存在形式及对晶界状态的影响[J].稀土,1983(04):58-68. |
[3] | 苏德达.原始组织对T10A钢奥氏体晶粒长大的影响[J].金属制品,2004(04):45-50. |
[4] | 毛卫民;赵新兵.金属的再结晶与晶粒长大[M].北京:冶金工业出版社,1994:236. |
[5] | Sellars C M;Whiteman J A.Recrystallization and grain growth in hot rolling[J].Metal Science Journal,1979(3-4):87-194. |
[6] | 钟云龙,刘国权,刘胜新,刘长胜,李光,何岳,钱红宝,李洪德,江玉祥.新型油井管钢33Mn2V的奥氏体晶粒长大规律[J].金属学报,2003(07):699-703. |
[7] | 杨庆祥,廖波,姚枚,刘建华,李向利.稀土对60CrMnMo钢奥氏体长大动力学的影响[J].中国稀土学报,1998(03):274-276. |
[8] | Sangho UHM;Joonoh MOON;Changhee LEE .Prediction Model for the Austenite Grain Size in the Coarse Grained Heat Affected Zone of Fe-C-Mn Steels: Considering The Effect of Initial Grain Size on Isothermal Growth Behavior[J].ISIJ International,2004(7):1230-1237. |
[9] | Vandermeer R A;Hu H .On the grain growth exponent of pure iron[J].Acta Metallurgica Et Materialia,1994,42(09):3071-3075. |
[10] | Ivasishin OM.;Semiatin SL.;Markovsky PE.;Shevchenko SV.;Ulshin SV. .Grain growth and texture evolution in Ti-6Al-4V during beta annealing under continuous heating conditions[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2002(1/2):88-96. |
[11] | P. A. MANOHAR;D. P. DUNNE;T. CHANDRA;C. R. KILLMORE .Grain Growth Predictions in Microalloyed Steels[J].ISIJ International,1996(2):194-200. |
[12] | Beynon J H;Sellars C M .Modeling microstrocture and its effects during multipass hot rolling[J].ISIJ International,1992,32(03):359-367. |
[13] | 朱兴元,陈邦文,林勤.稀土微合金化作用研究现状分析[J].钢铁研究,1999(04):60. |