采用经过驯化的HQ0211菌对高砷金矿进行氧化预处理-氰化提金实验研究.该矿石含金128.5 g/t,含砷16.84%(质量分数,余同),含硫21.72%,含铁26.62%,氰化浸出率只有29.35%,是典型的高砷难处理矿.经过细菌氧化预处理,金矿脱砷率达到96.2%,失重率达到43.9%.矿石的金氰化浸出率由原来的29.35%提高到92.57%,效果十分显著.
参考文献
[1] | Arpad E Torma;李纪归.生物湿法冶金的现状和未来的挑战[J].国外金属矿选矿,1990(10):28-32. |
[2] | 陈世琯.生物浸出及其在有色冶金中的应用[J].上海有色金属,2000(03):137-146. |
[3] | D. Morin;A. Lips;T. Pinches .BioMinE - Integrated project for the development of biotechnology for metal-bearing materials in Europe[J].Hydrometallurgy,2006(1/4):69-76. |
[4] | J.D. Batty;G.V. Rorke .Development and commercial demonstration of the BioCOP~(TM) thermophile process[J].Hydrometallurgy,2006(1/4):83-89. |
[5] | Demergasso C S;Galleguillos P P A;Escudero G L V et al.Molecular characterization of microbial populations in a low-grade copper ore bioleaching test heap[J].Hydrometallurgy,2005,80:241-153. |
[6] | R.B. Hawkes;P.D. Franzmann;J.J. Plumb .Moderate thermophiles including "Ferroplasma cupricumulans" sp. nov. dominate an industrial-scale chalcocite heap bioleaching operation[J].Hydrometallurgy,2006(1/4):229-236. |
[7] | A. Parker;C. Klauber;A. Kougianos .An X-ray photoelectron spectroscopy study of the mechanism of oxidative dissolution of chalcopyrite[J].Hydrometallurgy,2003(1/2):265-276. |
[8] | 杨洪英;杨立.细菌冶金学[M].北京:化学工业出版社,2006 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%