通过热模拟试验,研究了0.058%C-0.92%Mn-0.51%V钢在变形后等温过程中的组织变化规律及显微硬度变化规律,并用透射电镜研究了V(C,N)的沉淀析出规律.结果表明,变形后在650、700、750℃等温100 s时可获得单相铁素体组织,从而基本消除珠光体组织.等温转变过程中,铁素体先是主要沿奥氏体晶界形核,随后逐渐变为晶内形核.V(C,N)的沉淀析出存在两种形式:相间析出和随机析出.V(C,N)的相间析出消除了C元素在奥氏体中的富集,是获得单相铁素体组织的重要条件.

参考文献

[1] Misaharu Jitsukawa;Yoshihiro Hosoya.NKK'State - of - the - Art Flat - rolled Products Developed in the Last Decade[J].NKK Technical Review,2003:46-57.
[2] Zajac St.The Role of Nitrogen in Microalloyed Steels[J].Iron and Steel Society,1995(06):11-14.
[3] LAGNEBORG R.Influence of Processing Route and Nitrogen Content on Microstructure Development and Precipitation Hardening of V - microalloyed HSLA Steels[M].Pittsburg:The Metallurgical Society,1981
[4] Khalid F A;Edmonds D V.Interphase Precipitation in Microalloyed Engineering Steels and Model Alloy[J].Materials Science and Technology,1993:384-396.
[5] Smith R M;Dunne D P.Structure Aspects of Alloy Carbonitride Precipitation in Microalloyed Steels[J].Materials Forum,1988(11):166-181.
[6] Hirowo G SUZUKI;Mitsuru TANINO.Mechanism of Formation of Lined - up V4C3 Precipitates in Low Carbon Vanadium Steels[J].Transactions of the Iron and Steel Institute of Japan,1972(12):217-222.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%