针对内部爆炸加载的工业纯铁圆管和爆炸成形弹丸非常高的宏观塑性变形,对相应的微观组织进行了观察.结果表明:塑性变形时纯铁内发生动态回复和动态再结晶,这与冲击波引起的绝热温升和塑性变形功产生的绝热温升有关;动态回复和动态再结晶的软化作用使纯铁具有较高的塑性变形能力.

参考文献

[1] Worswick M J.Microstructure and fracture during high strain forming of iron and tantalum, shock wave and high strain rate phenomena in materials[M].[s. l.]:[s. n.],1992:87-95.
[2] 胡八一 .内部爆炸加载下钢管膨胀断裂研究[J].爆炸与冲击,1993,13(01):49-54.
[3] Murr L E .Residual microstructures in explosively formed tantalum penetrator[J].Scripta Metallurgica et Materialia,1994,31:297-302.
[4] BELYAKOV A .Substructural changes during hot deformation of an Fe - 26Cr ferritic stainless steel[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,2000,31:21-27.
[5] A.Iza-Mendia .Microstructural and Mechanical Behavior of a Duplex Stainless Steel under Hot Working Conditions[J].Metallurgical and Materials Transactions, A. Physical Metallurgy and Materials Science,1998(12):2975-2986.
[6] YANG Y .Localized superplastic behavior in α-titanium at high strain-rate[J].Scripta Metallurgica et Materialia,1995,33:219-224.
[7] Meyers M A.Dynamic behavior of materials[M].New York:wiley,1994
[8] Meyers M A .The attenuation of shock waves in Nickel[J].Materials Science and Engineering,1983,59:235-249.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%