对细晶Incone1718高温合金无中间层和加Ni箔中间层两种情况下的扩散连接进行了研究,分析了不同的连接温度、连接压力、连接时间等工艺参数对接头剪切强度的影响;通过SEM、EPMA和金相技术对接头微观组织和力学性能进行了分析.确定了获得优质接头的最佳工艺参数区间,即扩散连接温度T=1 050℃,连接压力P=20 MPa,连接时间t=45 min,选用Ni箔作为中间层,厚度为25 μm.

参考文献

[1] 李成功;傅恒志;于翘.航空航天材料[M].北京:国防工业出版社,2002
[2] Kashyap B.P.;Chaturvedi M.C. .ACTIVATION ENERGY FOR SUPERPLASTIC DEFORMATION OF IN718 SUPERALLOY[J].Scripta materialia,2000(5):429-433.
[3] Lu HJ.;Jia XC.;Zhang KF.;Yao CG. .Fine-grained pretreatment process and superplasticity for INCONEL718 superalloy[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2002(2):382-385.
[4] Liu R G;JIANG H M;JIANG Y .Study on superplastic deformation and mechanical behavior of alloy GH4169[J].Journal of Aerospace Materials and Technology,1998,28:36-38.
[5] Medeiros S C;Prasad Y V R K;Frazier W G;Srinivasan R .Microstructural Modeling of Dynamic Recrystallization in Hot Working of IN718 Superalloy[J].Materials Science and Engineering,2000,A293:198-207.