用反相微乳液法制备了壳聚糖-CdS复合纳米粒子,并考察了复合纳米粒子用量、光照条件和溶液pH值等因素对光催化降解甲基橙的影响.结果表明:在100 mL质量浓度为20 mg/L的甲基橙溶液中加入0.30 g复合纳米粒子,可以达到较好的光催化降解效果;甲基橙在光催化降解过程中最大吸收波长464 nm处的吸收峰迅速减弱,并最终消失,且在258 nm和455 nm处出现了新的吸收峰,说明甲基橙发生了降解;溶液pH值对光催化降解甲基橙有一定的影响,在弱酸性条件下降解效率较高;复合纳米粒子比普通CdS降解效率高,2 min时高出50%,400 min时高出21.3%.初步提出了复合纳米粒子光催化降解机理,复合纳米粒子的吸附作用是光催化降解作用的前置步骤.

参考文献

[1] KORGEL B A;MONBOUQUETTE H G .Quantum confinement effects enable photocatalyzed nitrate reduction at neutral pH using CdS nanocrystals[J].Journal of Physical Chemistry B,1997,101(25):5010-5017.
[2] LI Z;DU Y .Biomimic synthesis of CdS nanopartcles with enhanced luminescence[J].Materials Letters,2003,57(16-17):2480-2484.
[3] 李湛,杜予民,闻燕.模拟生物矿化制备壳聚糖/CdS半导体纳米复合膜[C].第三届甲壳素化学与应用研讨会论文集,2001:259-261.
[4] SABRINE F;LORENZA S;MARCOFABIO R .Size tailoring of CdS nanoparticles by different colloidal chemical techiniques[J].Colloids and Surfaces A:Physicochemical and Engineering Aspects,2001,177:3-4.
[5] BAC W;ABDULLAH R;MEHRA R K .Cysteine-mediated synthesis of CdS bionanocrystallites[J].Chemosphere,1998,37(02):363-385.
[6] SMITH P R;HDMAS J D;RICHARDSON D J et al.Photophysical and photochemical characterization of bacterial semiconductor cadmium sulfide particles[J].Journal of the Chemical Society,Faraday Transactions,1998,94(09):1235-1241.
[7] 王风贺,雷武,夏明珠,魏运洋,王风云.丙烯酰胺三元反相微乳液体系的制备及其聚合研究[J].材料科学与工艺,2006(01):54-56.
[8] 陈友存,叶信宇.纳米CdS微粒的制备、表征及光催化性质研究[J].安庆师范学院学报(自然科学版),2003(02):1-3.
[9] AL-QARADAWI S;SALMAN S R .Photocatalytic degradation of methyl orange as a modle compound[J].Journal of Photochemistry and Photobiology A:Chemistry,2001,148(1-3):161-168.
[10] BAIOCCHI C;BRUSSINO M C;PRAMAURO E et al.Characterization of methyl orange and its photocatalytic degradation products by HPLC/UV-VIS diode array and atmospheric pressure ionization quadrpole ion trap mass spectrometry[J].International Journal of Mass Spectrometry and Ion Processes,2002,214(02):247-256.
[11] MILLS A;WILLIAMS G .Methyl orange as a probe of the semiconductor-electrolyle interface in CdS suspensions[J].Journal of the Chemical Society,Faraday Transactions,1987,83:2647-2661.
[12] 陈炳稔.可再生甲壳质的吸附特性研究[M].广州:华南理工大学出版社,1998
[13] REUTERGARDH L B;IANGPHASUK M .photocatalytic decolourization of reactive AZO dye:A comparision between TiO2 and CdS photocatalysis[J].Chemosphere,1997,35(03):585-596.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%