本文讲述水口堵塞对生产和钢质的影响,指出水口堵塞的生成原因和防止措施.

参考文献

[1] 魏春新,王志英,张崇民.铝改硅镇静钢浇注钢包水口堵塞原因及预防措施[J].连铸,2001(03):36-38.
[2] L. A. Frank .Castability--from alumina to spinels[J].Iron & Steelmaker,1999(4):33-39.
[3] 卢盛意.连铸坯质量[M].北京:冶金工业出版社,2000
[4] G.M. Faulring.Inclusion Modification in semi - killid steels[J].Ironmaking and Steelmaking,1999(07):29.
[5] K. Mizuno;H. Todoroki;M. Noda .Effects of Al and Ca in Ferrosilicon Alloys for Deoxidation on Inclusion Composition in Type 304 Stainless Steel[J].Iron & Steelmaker,2001(8):93-101.
[6] R. Maddalena;R. Rastogi .Nozzle Deposits in Titanium Treated Stainless Steels[J].Iron & Steelmaker,2000(12):71-79.
[7] ADRIAN. Normanton;Brian patrick.Adrances in continuous casting technology[J].Ironmaking and Steelmaking,2000(04):260.