欢迎登录材料期刊网

材料期刊网

高级检索

采用两参数Weibull分布,对Nextel 720纤维强度及其分布进行了研究,并采用Kolmogorov非参数检验对其分布进行了检验.采用液相浸渍(硅溶胶、石英浆料和氮化硅浆料)对Nextel 720纤维进行处理,研究其对Nextel 720纤维强度的影响.结果表明,可用两参数Weibull分布表征纤维束强度分布.热处理使纤维强度急剧下降,且强度分散性变大.上浆后800℃处理,纤维束强度较高,Weibull模数高于原始纤维束;1000℃处理后,温度对纤维束的损伤严重,强度较低,但比不上浆相同温度处理纤维束强度高,分散性小.

参考文献

[1] S. Wu;L. Cheng;L. Zhang .Oxidation behavior of 3D Hi-Nicalon/SiC composite[J].Materials Letters,2006(25/26):3197-3201.
[2] 刘小瀛,张钧,张立同,徐永东,栾新刚.C/SiC复合材料应力氧化失效机理[J].无机材料学报,2006(05):1191-1196.
[3] ZOK Frank W;LEVI Carlos G .Mechanical Properties of Porous-Matrix Ceramic Composites[J].Advances in Engineering Materials,2001,3(1-2):15-23.
[4] Hiroki Fujita;Carlos G. Levi;Frank W. Zok .Controlling Mechanical Properties of Porous Mullite/Alumina Mixtures Via Precursor-Derived Alumina[J].Journal of the American Ceramic Society,2005(2):367-375.
[5] J.J.Haslam;K.E.Berroth .Processing and properties of an all-oxide composite with a porous matrix[J].Journal of the European Ceramic Society,2000(5):607-618.
[6] ANON.3M Nextel Textiles Product Description Brochure 3M[M].St.Paul,MN
[7] R.S.Hay;E.Boakye .Effect of coating deposition temperature on monazite coated fiber[J].Journal of the European Ceramic Society,2000(5):589-597.
[8] WILSON D M;LIEDER S L;LUENEBURG D C .Microstructure and high temperature properties of Nextel 720 fibers[J].Ceramic Engineering and Science Proceedings,1995,16(05):1005-1014.
[9] M. Dennis Petry;Tai-Il Mah .Effect of thermal exposures on the strengths of Nextel 550 and 720 filaments[J].Journal of the American Ceramic Society,1999(10):2801-2807.
[10] Konstantinos G. Dassios;Marc Steen;Constantina Filiou .Mechanical properties of alumina Nextel~(TM) 720 fibres at room and elevated temperatures: tensile bundle testing[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2003(1/2):63-72.
[11] CHI Zhi-fan;CHOU Tsu-Wei;SHEN Guo-yi .Determination of single fibre strength distribution from fibre bundle testings[J].Journal of Materials Science,1984,19(10):3319-3324.
[12] Lange FF.;Evans AG.;Tu WC. .PROCESSING OF DAMAGE-TOLERANT, OXIDATION-RESISTANT CERAMIC MATRIX COMPOSITES BY A PRECURSOR INFILTRATION AND PYROLYSIS METHOD[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,1995(1/2):145-150.
[13] KANKA B;SCHNEIDER H .Aluminosilicate fiber/mullite matrix composites with favorable high-temperature properties[J].Journal of the European Ceramic Society,2000,20:619-623.
[14] She JH.;Mechnich P.;Schneider H.;Schmucker M.;Kanka B. .Effect of cyclic infiltrations on microstructure and mechanical behavior of porous mullite/mullite composites[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2002(1/2):19-24.
[15] S.L. Fok;B.C. Mitchell;J. Smart .A numerical study on the application of the Weibull theory to brittle materials[J].Engineering Fracture Mechanics,2001(10):1171-1179.
[16] Pickering K.L.;Murray T.L. .Weak link scaling analysis of high-strength carbon fibre[J].Composites, Part A. Applied science and manufacturing,1999(8):1017-1021.
[17] J. Andersons;R. Joffe;M. Hojo .Glass fibre strength distribution determined by common experimental methods[J].Composites science and technology,2002(1):131-145.
[18] 吴喜之;王兆军.非参数统计方法[M].北京:高等教育出版社,1996:151-167.
[19] F. Deleglise;M.H. Berger;D. Jeulin .Microstructural stability and room temperature mechanical properties of the Nextel 720 fibre[J].Journal of the European Ceramic Society,2001(5):569-580.