高级检索

研究T700/9916碳纤维增强复合材料(CFRP)层合板在湿热环境下的吸湿行为.通过测试CFRP层合板在T=70℃恒温水浴和T=70℃相对湿度为98%,91%和84%的环境下的吸湿性能,获得吸湿曲线.结果表明水浸试样相对质量增量趋于平衡时,其他各组试样的相对质量仍线性增加.使用一维Fick模型对实验结果进行分析,得到材料的理论吸湿数据比实验结果整体偏小.通过实验和有限元模拟相结合的方法计算获得材料的扩散率和溶解度,并对不同条件下的吸湿行为进行模拟,模拟结果与实验结果吻合较好,说明通过模拟能够获得材料的长期吸湿动力学曲线和试样内部的水分分布情况.

参考文献

[1] 陈祥宝.先进树脂基复合材料的发展[J].航空材料学报,2000(01):46-54.
[2] US Army Research Laboratory,Weapons and Materials Research Directorate.MIL-HDBK17-1F Composite materials handbook[M].Philadelphia:the Document Automation and Production Service,2002
[3] MCKAGUE E L;REYNOLDS J D;HALKIAS J E .Life assurance of composite structures:AFML-TR-75-51:Vol 1[R].Ohio:AFML(LC),Wright-Patterson AFB,1975.
[4] BONNIAU P;BUNSELL A R .A comparative study of water absorption theories applied to glass epoxy composites[J].Journal of Composite Materials,1981,15(03):272-293.
[5] IMAZ J J;RODRIGUEZ J L;RUBIO A .Hydrothemal environment influence on water diffusion and mechanical behavior of carbon fibre/epoxy laminates[J].Journal of Materials Science Letters,1991,10(11):662-665.
[6] 郑路,常新龙,赵峰,张博.湿热环境中复合材料吸湿性研究[J].纤维复合材料,2007(02):37-39.
[7] SHEN C H;SPRINGER G S .Moisture absorption and desorption of composite materials[J].Journal of Composite Materials,1976,10(01):2-20.
[8] Pavankiran Vaddadi;Toshio Nakamura;Raman P. Singh .Inverse analysis for transient moisture diffusion through fiber-reinforced composites[J].Acta materialia,2003(1):177-193.
[9] 孙丽 .纤维增强环氧树脂基复合材料吸湿行为的有限元研究[D].天津大学,2007.
[10] ASTM D5229/D 5229M.ASTM D5229/D 5229M.Standard test method for moisture absorption properties and equilibrium conditioning of polymer matrix composite materials[S].PA:ASTM International,1992.
[11] ABAQUS User Manual,Dassault Systems[M].Rhode Island:H:Bbitt,karlsson & Sorensen,Inc,2008
[12] MERCIER J;BUNSELL A;CASTAING P .Characterization and modeling of aging of composites[J].Composites (A),2008,39(02):428-438.
[13] BOUKHOULDA B F;ADDA-BEDIA E;MADANI K .The effect of fiber orientation angle in composite materials on moisture absorption and material degradation after hydrothermal ageing[J].Computers & Structures,2006,74(04):406-418.