综述了高温结构陶瓷材料在高温条件下结晶机理及氧化理论,对各种理论模型进行了评介.其中重点介绍了Si-C-(O)-(N)体系的"无定型-成核-晶粒长大"结晶机理和Si-C-N体系的"分离-分解-结晶"结晶机理;并具体介绍了Si-C-N-O和Si-(B)-C-N高温氧化机理.

参考文献

[1] 彭志坚,司文捷,林仕伟,苗赫濯.用有机硅聚合物制备高温结构陶瓷材料研究进展[J].无机材料学报,2001(05):779-790.
[2] Ray Johnson D;Stiegler James O .Structural ceramics R · D[J].Current Advances in Materials and Processes,1990,9:55-56,59-61.
[3] 杨一明;冯春祥 .用一种简易方法制造碳化硅成形体[J].宇航材料工艺,1998,4:22-26.
[4] 王晓君;刘凤荣;张长瑞 .C/SiC复合材料的制备及性能研究[J].复合材料,1991,8(02):77-83.
[5] Ralf Riedel;Passing G;Herbert Schonfelder;Brook R J .Synthesis of dense silicon-based ceramics at low temperatures[J].Nature,1992,355:714-717.
[6] 苏波;吴小进;刘凤荣;王兴业 .低分子聚硅氮烷(LPSZ)/二乙烯基苯(DVB)的交联及其对裂解产物的影响[J].材料研究学报,1994,8(02):163-168.
[7] 李永清;陈朝晖 等.先驱体转化制备SiC/Si3N4复相陶瓷异型体成型工艺研究[J].宇航材料工艺,1996,6:1-9.
[8] 宋永才,王岭,冯春祥.聚碳硅烷的合成与特性研究[J].高分子材料科学与工程,1997(04):30-33.
[9] Eddy Vanswijgenhoven;John Holmes;Martine Wevers;Andy Szweda .The influence of loading frequency on the high-temperature fatigue behavior of a nicalon-fabric-reinforced polymer-derived ceramic-matrix composite[J].Scripta materialia,1998(12):1781-1788.
[10] Nikhilesh Chawla;Tur Yahya K et al.High-frequency fatigue behavior of woven-fibric-reinforced polymer-derived ceramic-matrix composites[J].Journal of the American Ceramic Society,1998,81(05):1221-1230.
[11] 龙剑峰 .用有机硅聚合物制造陶瓷材料[J].有机硅材料及应用,1999,13(06):23-26.
[12] Xin-Bo He;Xin-Ming Zhang;Chang-Rui Zhou;An-Chen Zhou .Microstructures and mechanical properties of Cf/SiC composites by precursor pyrolysis-hot pressing[J].Materials Science and Engineering,2000,A284:211-218.
[13] DELVERDIER O;Monthioux M;Mocaer D;Pailler R .Thermal behavior of polymer-derived ceramicsⅠ SiC and Si-C-O systems from both commercial and new polycarbosilane (PCS) precursors[J].Journal of the European Ceramic Society,1993(12):7-41.
[14] DELVERDIER O;Monthioux M;Mocaer D.Thermal behavior of polymer-derived ceramics Ⅳ Si-C-N-O fibers form an oxygen-cured polycarbosilazane[J].Journal of the European Ceramic Society,1994:313-325.
[15] Monthioux M;Delverdier O .Thermal behavior of (orgnosilicon) polymer-derived ceramicsⅤmain facts and trends[J].Journal of the European Ceramic Society,1996(16):721-737.
[16] H.Muller;H.-J.Kleebe;D.Suttor .Microstructure evaluation of polymer-derived Si-C-N-Ceramics characterised by scanning- and transmission electron microscopy[J].Key engineering materials,1997(3):2005-2008.
[17] Kleebe HJ. .Microstructure and stability of polymer-derived ceramics; The Si-C-N system[J].Physica Status Solidi, A. Applied Research,1998(1):297-313.
[18] Ziegler G;Kleebe H J;Motz G;Müller H,Tra 1 S,Weibelzahl W .Synthesismicrostructure and properties of SiCN ceramics prepared from tailored polymers[J].Materials Chemistry and Physics,1999,61:55-63.
[19] Kleebe H J;Motz G;Ziegler G .Microstructure and properties of polymer-derived SiCN ceramics[J].Key Engineering Materials,1999,175:57-68.
[20] Christoph Haluschka;Hans-Joachim Kleebe;Rainer Franke;Ralf Riedel .Silicon carbonitride ceramics derived from polysilazanes Part Ⅰ investigation of compositional and structural properties[J].Journal of the European Ceramic Society,2000,20:1355-1364.
[21] Georges Chollon .Oxidation behavior of ceramic fibers from the Si-C-N-O system and related sub-systems[J].Journal of the European Ceramic Society,2000,20:1959-1974.
[22] Li-Anne Liew;Wenge Zhang;Victor M. Bright;Linan An;Martin L. Dunn;Rishi Raj .Fabrication of SiCN ceramic MEMS using injectable polymer-precursor technique[J].Sensors and Actuators, A. Physical,2001(1/2):64-70.
[23] Ralf Riedel et al.A silicoboron carbonitride ceramics stable to 2000℃[J].Nature,1996,382:796-798.
[24] RAJ R;An L;Shah S;Riedel R,Fasel C,Kleebe H-J .Oxidation kinetics of an amorphous silicon carbonitride ceramics[J].Journal of the American Ceramic Society,2001,84(08):1803-1810.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%