采用粉末冶金法制备了φ300mm的15%(体积分数)SiCp/Al复合材料坯锭,研究了热挤压、锻造后的材料力学性能以及断裂特点.结果表明,该材料的弹性模量在97 GPa、拉伸强度保持在550 MPa的水平下,延伸率仍高达7%左右,旋转弯曲疲劳强度在250~290 MPa范围内,断裂韧性为25 MPa·m1/2,冲击韧性为62.5 kJ/m2.与棒材挤压态相比,T4态复合材料拉伸强度和屈服强度分别提高66.7%和100%,但塑性保持在同一水平.断口观察表明,挤压态复合材料以基体韧性断裂为主要形式,而T4态复合材料除了基体韧性断裂外,还存在SiC颗粒断裂现象.挤压棒材锻造后有利于提高材料的横向强度.

参考文献

[1] Geiger A L;Walker J A.The processing and properties of discontinuously reinforced aluminum composites[J].Journal of The Minerals,Metals & Materials Society,1991(08):8-15.
[2] Benji Maruyama;Warren H. Hunt Jr. .Discontinuously reinforced aluminum: current status and future direction[J].JOM,1999(11):59-61.
[3] Mark Hull .Commercial success for MMCs[J].Powder Metallurgy,1998(1):25-26.
[4] AMC .Leading edge MMCs and powder materials[J].Powder Metallurgy,1997,40(02):102-103.
[5] Mekimpson M G;Pohlenz E L;Thompson S R.Evaluating the mechanical properties of commercial DRA[J].Journal of The Minerals,Metals & Materials Society,1993(01):26-29.